Heidelberg researchers have successfully developed a new generation of biocompatible materials for additive manufacturing. Microalgae such as the diatom Odontella aurita and the green alga Tetraselmis striata, which are rich in lipids and photoactive pigments, are particularly suitable as “biofactories” for producing sustainable materials for 3D laser printing. An international research team led by Professor Dr. Eva Blasco from the Institute for Molecular Systems Engineering and Advanced Materials (IMSEAM) at Heidelberg University has, for the first time, manufactured inks for printing complex biocompatible 3D microstructures from raw materials extracted from these microalgae. These microalgae-based materials could potentially be used in the future as the basis for implants or scaffolds for 3D cell cultures.
Among the additive manufacturing techniques, two-photon 3D laser printing offers particular advantages for manufacturing at the micro- and nanoscale. Owing to its remarkable resolution, it finds application in numerous fields including optics and photonics, microfluidics, and biomedicine. The process involves focusing a laser beam on a liquid, photoreactive resin, a so-called “ink”. At the focal point, the laser light activates special molecules known as photoinitiators and triggers a chemical reaction, causing local solidification of the ink.
To date, petrochemical-based polymers have been mainly used as inks for this highly precise 3D laser printing process. However, these polymers contribute to the depletion of fossil fuels and the emission of greenhouse gases and can also contain toxic components, as Professor Blasco points out. Microalgae are particularly well suited as “biofactories” for the production of sustainable materials for 3D printing due to their rapid growth rate, CO2-fixation during cultivation, and biocompatibility. “Despite their advantages, microalgae have hardly been considered as raw materials for light-based 3D printing,” says Professor Blasco, whose group conducts research at the interface of macromolecular chemistry, materials science, and 3D nanofabrication.
The research team succeeded for the first time in extracting biocompatible materials for high-resolution 3D laser printing from microalgae. For their experiments, the researchers selected two species – the diatom Odontella aurita and the green alga Tetraselmis striata – that contain particularly high levels of lipids in the form of triglycerides. The team extracted the triglycerides and functionalized them with acrylates to facilitate rapid curing under light irradiation. The photoactive green pigments present in the microalgae proved to be suitable as photoinitiators. When exposed to light, they trigger the chemical reaction that solidifies the ink into a three-dimensional structure. “In this way we avoid using potentially toxic additives like the photoinitiators used in conventional inks,” explains first author Clara Vazquez-Martel, a doctoral candidate in Eva Blasco’s research team at IMSEAM.
Using the new ink system, the researchers were able to produce different 3D microstructures with high precision, exhibiting complex features such as overhanging roofs and cavities. Using cell culture experiments, the researchers also investigated the biocompatibility of the microalgae-based inks. They prepared 3D microscaffolds on which the cells were cultured for about 24 hours. They observed a survival rate of almost 100 percent. “Our results open up new possibilities not only for more sustainable 3D printing with light, but also for life science applications – from 3D cell cultures to biocompatible implants,” says Professor Blasco.
For more information: Heidelberg University