Members of Lawrence Livermore National Lab’s Additive Manufacturing Initiative, Calif, are among a group of researchers who have developed 3D printed materials with a unique property—instead of expanding when heated, they shrink. LLNL engineers, along with scientists from the University of Southern California, MIT, and UCLA, 3D printed lightweight metamaterials with negative thermal expansion that can be “tuned” to shrink over a large range of temperatures.
“This is a new version of a printing method we have developed and used in the past. We used it to create a thermomechanical metamaterial that may enable applications not possible before,” says principal investigator Chris Spadaccini, director of LLNL’s Center for Engineered Materials and Manufacturing. “It has thermomechanical properties not achievable in conventional bulk materials.”
Researchers demonstrate a bi-material microlattice structure, printed from polymer and a polymer/copper composite material that can flex inward, causing the structure to contract when exposed to heat over a range of tens to hundreds of degrees. This study may be the first experimental demonstration showing large tunability of negative thermal expansion (NTE) in three Cartesian directions of microlattice structures.
Possible applications for the metamaterials could come in securing parts that tend to move out of alignment under varying heat loads, including microchips and high-precision optical mounts, according to researchers.
“Traditionally, the way you compensate for (thermal mismatches) is with active control or heating and cooling,” Spadaccini says. “But what if you could design a material that would hold the object and passively adjust to local temperature changes?”
Jonathan Hopkins, assistant professor of mechanical aerospace and engineering at UCLA, designed similar structures in a separate study using a human interaction-based approach rather than computer-driven.
“The interesting thing (about the structure) is it’s made of two different materials, beams and void space,” Hopkins explains. “When you heat it, as long as one of the beams expands more than the others, then the connecting points between each unit cell pulls inward and makes the overall lattice pull inward. It’s an immediate thermal contraction, which is the unique thing about it.” The thermal expansion also can be zero or positive depending on how the geometry and topology of the structure are engineered, Hopkins notes.
A team at MIT, led by associate professor of mechanical engineering Nicholas Fang, 3D-printed the microlattice structures using a projection microstereolithograpy process. USC assistant professor of civil and environmental engineering Qiming Wang worked for Fang as a postdoc.
“Here we take advantage of projection microstereolithography 3D printing, but this time we expanded the system to be able to fabricate multimaterials; after you print out one material you switch to another,” Wang says. “The challenge is you have to eliminate contamination between materials. If you don’t wash out the residue after every layer, two materials will be mixed up.”
Wang says the microstructured metamaterial could be used in dental fillings, which tend to move or crack when a person eats something hot, to fill in small gaps in bridges or buildings that are normally left open to account for thermal expansion, or in precision devices such as atomic-force microscopes.
“The problem we’re treating is a thermal mismatch problem,” Wang says. “These materials have different thermal expansion coefficients, so once we increase the temperature, they interact with each other and pull inward, so the overall structure’s volume decreases. The next step is to fabricate zero thermal expansion materials that could also solve these problems.”
The study is part of a five-year Defense Advanced Research Projects Agency (DARPA) Defense Sciences Office (DSO) program to research materials with controlled microstructure architecture.
Other collaborators include LLNL engineer Julie Jackson, and MIT postdoc Qi Ge.
Image caption — A bi-material microlattice structure, 3D printed from polymer and a polymer/copper composite material, can flex inward, causing the structure to contract when exposed to heat over a range of tens to hundreds of degrees.