Scientists worldwide are striving to scale quantum technologies, which hinges on reliably generating qubits—the basic units of quantum information. One promising material for this is hexagonal boron nitride (h-BN), a two-dimensional substance known for hosting solid-state single-photon emitters (SPEs). These atomic structures can emit individual photons, making them strong candidates for building scalable quantum systems.
In a study, researchers at Rice University and collaborators at Oak Ridge National Laboratory and the University of Technology, Sydney report the first demonstration of low noise, room-temperature quantum emitters in h-BN made through a scalable growth technique.
The researchers used pulsed laser deposition (PLD) to synthesize h-BN films, deliberately adding carbon atoms during the deposition process. The carbon gets woven into the atomic lattice of h-BN in a way that generates so-called defects or irregularities. These defects are a feature rather than a flaw, functioning as robust and reliable SPEs.
“Our work demonstrates a scalable method to create high-performance SPEs in h-BN, offering a major step toward practical quantum light sources,” said Arka Chatterjee, a postdoctoral researcher in the lab of Rice electrical engineer Shengxi Huang. “This breakthrough paves the way for integrating quantum emitters into real-world photonic and quantum information systems.”
The equivalent to the qubit in classical computing is the bit, a contraction of “binary digit,” meaning it can have one of two values, either 1 or 0. The bit makes present computing and communication technologies possible, and the main way of embedding this binary state into physical systems in our current devices is electrical charge: In transistors and computing chips, for instance, the presence or absence of charge determines the logical value of the bit and serves to encode information. Reliable SPEs like those developed in this study are key to encoding and manipulating qubits in emerging quantum computing and communication platforms.
To work well, SPEs must perform reliably and uniformly, namely producing only a single photon of the same kind at a time ⎯ a tall order for structures that are commonly referred to as “defects” or “impurities.”
“We hypothesized that introducing carbon during the direct growth of h-BN films could create defect centers capable of emitting highly pure single photons at room temperature,” said Chatterjee, who is a first author on the study.
To test this hypothesis, the team turned to the lab of Rice materials scientist Pulickel Ajayan, where research scientist Abhijit Biswas used PLD to create centimeter-scale, carbon-doped h-BN thin films. The method offers several advantages, including PLD’s low-temperature requirements and the ability to integrate doping as part of a one-step synthesis process.
“Prior attempts to create stable h-BN emitters were limited by high-temperature synthesis or postprocessing steps that compromised purity and reproducibility,” said Huang, an associate professor of electrical and computer engineering and materials science and nanoengineering at Rice. “Our method overcomes these barriers by integrating doping and synthesis in a single, scalable step.”
Once the films were ready, the researchers tested their properties using photoluminescence spectroscopy, photon correlation measurements and theoretical modeling. These analyses revealed that the carbon-doped h-BN films had “exceptionally pure and stable SPEs, indicating near-ideal single-photon emission,” Chatterjee said.
“The emitters also exhibit high brightness, strong polarization and robust photostability during continuous operation,” he said, adding that first-principles calculations identified the carbon-induced defect structures as the origin of the emission.
The findings could enable the integration of SPEs into chip-based quantum devices and sensors, finally ushering in the much-anticipated transition to quantum-based technologies for communication, information processing and sensing.
“The combination of purity, scalability and operational stability sets a new benchmark and resolves long-standing challenges in the field,” Huang said.
For more information: Science Advances
Image: Arka Chatterjee is a first author on a study published in Science Advances and a postdoctoral researcher in the lab of Rice electrical and computer engineering professor Shengxi Huang. (Photo by Jeff Fitlow/Rice University.)