Researchers at UC San Diego have developed a straightforward yet effective technique using scanning electron microscopy to evaluate lithium metal battery performance, potentially speeding up the creation of safer, longer-lasting, and more energy-dense batteries for electric vehicles and large-scale energy storage. Lithium metal batteries can store twice the energy of current lithium-ion batteries, which could significantly extend the range of electric cars and the battery life of devices. However, achieving this requires controlling how lithium deposits during charging; uniform deposits lead to longer battery life, while uneven deposits form dangerous dendrites that can cause short circuits and battery failure.
Historically, researchers have largely determined the uniformity of lithium deposits by visually assessing microscope images. This practice has led to inconsistent analyses between labs, which has made it difficult to compare results across studies.
“What one battery group may define as uniform might be different from another group’s definition,” said study first author Jenny Nicolas, a materials science and engineering Ph.D. candidate at the UC San Diego Jacobs School of Engineering. “The battery literature also uses so many different qualitative words to describe lithium morphology — words like chunky, mossy, whisker-like and globular, for example. We saw a need to create a common language to define and measure lithium uniformity.”
To do so, Nicolas and colleagues — led by Ping Liu, professor in the Aiiso Yufeng Li Family Department of Chemical and Nano Engineering at the UC San Diego Jacobs School of Engineering — developed a simple algorithm that analyzes how evenly lithium is spread across scanning electron microscopy (SEM) images. The researchers used SEM because it offers detailed images of battery electrodes by capturing 3D surface features as 2D grayscale images — it is also a widely used technique in battery research.
To use their method, the team first takes SEM images of battery electrodes and converts them to black and white pixels. The white pixels represent the topmost lithium deposits in the sample and black pixels represent either the substrate or inactive lithium. The images are divided into multiple regions, and the algorithm counts the number of white pixels in each, then calculates a metric called the index of dispersion (ID).
“The index of dispersion is a measure of lithium uniformity,” Nicolas explained. “The closer it is to zero, the more uniform the lithium deposits. A higher value means less uniformity and more clustering of lithium particles in certain areas.”
The team first validated the method on 2,048 synthetic SEM images with known particle size distributions. The ID measurements aligned with the ground-truth distributions, which confirmed the method’s accuracy. The team then applied the method to real electrode images to analyze how lithium morphology changes over time under different cycling conditions. They found that as batteries cycled, the ID increased — indicating more uneven lithium deposits. Meanwhile, the energy required for lithium to deposit increased — a sign of degradation. In addition, the researchers found that local peaks and dips in the ID consistently appeared just before cells failed. Such peaks and dips could serve as an early warning sign of short circuits.
A big advantage of this method is that it is accessible. Battery researchers already use SEM imaging as part of their studies, Nicolas noted, and they can use the simple algorithm presented here to calculate the ID from the data they already collect.
“Our tool can be employed as a low-hanging fruit for researchers to take their analysis to the next level by utilizing image analysis to its fullest potential,” she said.
For more information: Proceedings of the National Academy of Sciences
Image: Scanning electron microscopy (SEM) images are already a common staple of battery research. Now, they can be paired with a simple algorithm to enable better prediction of lithium metal battery performance and failure. Credit: Jenny Nicolas et al.