Functionalization of fiber-reinforced plastic composites by thermal spraying

In this video, Fraunhofer’s thermal spraying group demonstrates how thermal spraying can be successfully used to apply multilayer heating systems with fiber-reinforced plastic composites so they can be used in applications previously dominated by metals.