Self-organizing steel balls explain metal heat treatment

 

Video description

This video from Steve Mould explains how the size of the grains affects the physical properties of the metal, like hardness, toughness, strength, mailability, ductility, and plasticity. Heating a metal can change the size of the grains. This ball-bearing model demonstrates annealing.