Battelle, Columbus, Ohio, is teaming with Rare Earth Salts (RES), Beatrice, Neb., on a project to extract rare earth oxides from coal fly ash, converting them to the high purities necessary for a saleable product. The project, Recovery of High Purity Rare Earth Elements (REEs) from Coal Ash via a Novel Separations Process, is sponsored by the U.S. Department of Energy’s National Energy Technology Laboratory.
The two organizations will advance the development of REE processing by combining the RES novel separation and purification process and Battelle’s Acid Digestion Process. Under this project, they will validate that they can generate environmentally benign and economically sustainable rare earth products from domestic coal ash sources at purities above 90 percent.
The total funding for the project is about $875,000.
Battelle’s Acid Digestion Process selectively leaches REE from the coal fly ash. It is unique in that the chemicals are almost entirely recycled instead of being lost to leaching during the process. This approach dramatically reduces costs, enables the exclusion of key contaminants, and provides a concentrated source of REEs along with other co-products. This process was originally used by Battelle to sustainably and safely disarm expired artillery munitions.
“This is an important project to prove the viability of this approach,” says Rick Peterson, Battelle Research Scientist. “The need to recover Rare Earth Elements in the United States is of national importance, since so much of the capacity to produce these critical materials lies outside the United States.”
RES’ proprietary separation technology is cost efficient and environmentally friendly. The company recycles its manufacturing inputs so virtually no waste is created, making RES the most sustainable producer of rare earth oxides globally. RES began commercial production of rare earth oxides at its Nebraska-based facility earlier this year with a standard purity of 99.9%.
“Our technology positions us to be a primary producer of consistent, low-cost, rare earth oxides to Western economies,” said Cameron Davies, Chief Executive Officer of RES. “As we seek additional sources of domestic rare earth feedstock, coal fly ash presents a promising opportunity. Battelle is a world-class partner, and we look forward to working together to meet the objectives of the U.S. Department of Energy.”