Wall Colmonoy, Madison Heights, Mich., is providing solutions to increase the lifetime of key operational equipment for U.K. steel manufacturers by laser cladding reheat furnace skid posts with Colmonoy 625. The coating of skid posts offers substantial advantages such as:
- Excellent resistance against hot gas corrosion
- Substantial cost savings vs. replacement of the whole part
- Heavily reduced downtime
The reheat furnace is a challenging environment due to the extreme conditions that the skid posts operate in where it is subject to continuous high temperature, corrosive gases and mechanical fatigue.
Downtime in this part of the manufacturing process results in significant maintenance costs and frustrating interruptions in the manufacture and supply of hot rolled coil for further downstream processing. The cladding of these skid posts with Colmonoy 625 provides protection against sulfur-induced hot gas corrosion which causes failure of the post and exposes the water-cooling system.
Colmonoy 625 has larger additions of chromium and molybdenum which protects against a range of corrosion mechanisms in atmospheres that would cause failure in lesser alloys. This solution can be applied to any industry that suffers with high temperature corrosion of furnace assets.
The steel producer turned to Wall Colmonoy for a cost-effective solution to their issues. Aerobraze Business Development Manager Dr. Lewis Berry stated “The coating of skid posts with Colmonoy 625 will generate a significant increase in lifetime in a very challenging operational environment and improve the stability of the process. Colmonoy 625 is an alloy that can be applied via a range of different techniques to suit the demands of the application.”
Image – Refurbished Furnace Skid Posts Clad in Colmonoy 625
For more information:
Wall Colmonoy
https://www.wallcolmonoy.com/