Seco/Warwick, Poland, will deliver an innovative AFT process line to Aalberts Surface. The delivery to the Dzierżoniów hardening plant includes a third main furnace, tempering furnace, and an endothermic atmosphere generator as well as loading and unloading devices along with the auxiliary infrastructure.
“This contract covers a main AFT type atmosphere furnace, intended for carburizing, hardening, nitrocarburizing and annealing processes,” explained Piotr Skarbiński, vicepresident, Business Segment Atmosphere Furnaces, SECO/WARWICK Group. “The furnace is perfect for manufacturing processes for various transmission components, enabling the use of both conventional load arrangements with modular accessories (mesh, grids or “cross-bars”) as well as hardening baskets” – P. Skarbiński added.
Dzierżoniów plant was established in 2014 and is one of the most modern commercial hardening plants in the region. They are a supplier primarily for the automotive industry, but also for the wide machinery industry.
Read further here