A team from the Tulane University School of Science and Engineering has developed a new family of two-dimensional materials that researchers say has promising applications, including advanced electronics and high-capacity batteries.
Led by Michael Naguib, an assistant professor in the Department of Physics and Engineering Physics, the study has been published in the journal Advanced Materials.
“Two-dimensional materials are nanomaterials with thickness in the nanometer size and lateral dimensions thousands of times the thickness,” Naguib said. “Their flatness offers unique set of properties compared to bulk materials.”
The name of the new family of 2D materials is transition metal carbo-chalcogenides, or TMCC. It combines the characteristics of two families of 2D materials — transition metal carbides and transition metal dichalcogenides.
Naguib said the latter is a large family of materials that has been explored extensively and found to be very promising, especially for electrochemical energy storage and conversion. But he said one of the challenges in using them is their low electrical conductivity and stability.
On the other hand, he said, transition metal carbides are excellent electrical conductors with much more powerful conductivity. Merging the two families into one is expected to have immense potential for many applications such as batteries and supercapacitors, catalysis, sensors and electronics.
“Instead of stacking the two different materials like Lego building blocks with many problematic interfaces, here we develop a new 2D material that has the combination of both compositions without any interface,” said Naguib.
“We used an electrochemical-assisted exfoliation process by inserting lithium ions in-between the layers of bulk transition metals carbo-chalcogenides followed by agitation in water,” said Ahmad Majed, the first author of the article and a doctoral candidate in Materials Physics and Engineering at Tulane working in Naguib’s group.
Unlike other exotic nanomaterials, Majed said, the process of making these 2D TMCC nanomaterials is simple and scalable.
For more information: Tulane University