Constellium, Paris, is entering into an agreement to provide Aheadd CP1, one of its proprietary additive manufacturing (AM) powder solutions, to Morf3D Inc., a subsidiary of Nikon Corp. specializing in AM optimization and engineering for the aviation, space, and defense industries.
“We are very excited to partner with Morf3D, a leading company in additive manufacturing, on the qualification and development of applications using our Aheadd CP1 aluminium powder,” said Alireza Arbab, head of additive manufacturing for Constellium. “Constellium recognized a gap in aluminium powder options for laser powder bed fusion (LPBF) and has developed new powders specifically for this AM process. We are confident that this program will highlight the benefits of Aheadd CP1 and help set new standards for aluminium component production using LPBF.”
Read further here.