Seco/Warwick, Poland, will supply a Vector vacuum furnace to Atlas Autos Ltd, the largest manufacturer of motorcycle parts in Pakistan. The solution is intended for hardening and tempering processes, and its design will allow for gas cooling elements and dies for parts used in automotive production.
The vacuum furnace on order is a Vector, the proven design for precision heat treatment with an effective work zone measuring 600 x 600 x 900 mm – the most popular size for tool and die production. The solution will be used for special large-size die production.
They can be used for most standard hardening, tempering, annealing, solution heat treatment and brazing processes. However, for each application, the furnace can be adapted to the recipient’s individual requirements and thus, a specific industry. This time, the furnace, which will be delivered to Atlas Autos in the second half of 2022, is the solution most often chosen by SECO/WARWICK customers. The heat treatment will be applied to dies to produce car and motorcycle parts. The Vector will be utilized for hardening and tempering process implementation.
Read further here.