A research team from the University of Tennessee, Knoxville, and Eastman, developed a new method to ensure consistency and quality in rubber manufacturing. Their novel process—which goes beyond optical microscopy—is likely to show real-world impact on material sustainability and durability for products such as car tires.
As consumers in the U.S. and around the globe are increasingly incentivized toward electric vehicles (EVs)and away from fossil-fuel reliance, current EV users have uncovered an unexpected maintenance issue. Due to the combination of higher weight and higher torque, EVs put more pressure on standard tires, causing them to degrade 30% faster than tires on internal-combustion vehicles.
UT’s Fred N. Peebles Professor and IAMM Chair of Excellence Dayakar Penumadu, along with electrical engineering graduate student Jun-Cheng Chin, postdoctoral researcher Stephen Young and three Eastman scientists, recently published research aimed at resolving one of rubber manufacturing’s most common challenges: identifying flaws in the material.
Rubber contains additives such as zinc oxide and sulfur that work to improve strength, elasticity, and other favorable traits. When the ingredients are not distributed evenly throughout a rubber product such as a car tire, the material will contain flaws that cause the product to degrade prematurely.
“If components such as sulfur do not disperse well, that generates localized hard spots,” said Penumadu. “That hard stuff attracts a lot of mechanical and thermal stresses, making the material degrade prematurely.”
Even a flaw the width of a human hair can decrease the life span of a large rubber component such as a car tire.
fracture mechanics—aimed at identifying and studying such flaws—is critical to understanding how the material will perform. Yet finding such flaws before they cause problems is an issue that has long plagued the rubber industry.
“The current industry approach is to cut out a small sample of rubber, then observe it under an optical microscope,” Penumadu said. “Not only is this tedious and destructive, it’s unreliable. It requires you to guess beforehand where, in an opaque sample, you need to check for inconsistencies.”
In addition, optical microscopes cannot differentiate between rubber components—for example, sulfur and zinc oxide both appear as white specks.
Penumadu’s team has overcome this issue by switching from optical analysis to x-ray computed tomography. X-rays that pass through the sample are scattered and absorbed differently depending on the materials they strike. A computer then reconstructs a digital 3D model of the rubber’s interior.
“This is a very important point,” Penumadu said. “XCT lets us see the inside of the material noninvasively, and we can actually see the distribution of each component.”
The application of this new method increases the rubber industry’s ability to view and predict flaws and will ultimately lead to more consistent quality and longer-lasting rubber products.
In October the team received the 2021 Publication Excellence Award from the Journal of Rubber Chemistry and Technology for their groundbreaking paper, “Sulfur Dispersion Quantitative Analysis in Elastomeric Tire Formulations by Using High Resolution X-Ray Computed Tomography,” which discusses the new XCT method and their research findings.
Image – Tires photo courtesy of Unsplash/CC0 Public Domain.
************
For more information: