Asylum Research, an Oxford Instruments company, Santa Barbara, Calif., announces Contact Resonance Viscoelastic Mapping Mode, an option available exclusively for Asylum’s Cypher and MFP-3D Atomic Force Microscopes. Contact Resonance (CR) enables high resolution, quantitative imaging of both elastic storage modulus and viscoelastic loss modulus. The technique is particularly well suited for characterizing moderate to high modulus materials in the range of about 1 to 200 GPa for materials such as composites, thin films, ceramics, and metals. Hardware and software developments have made contact resonance imaging significantly faster, more quantitative, simpler to use, and applicable to a wider range of materials.
“An important feature of contact resonance imaging is that it characterizes the full viscoelastic response of materials,” noted Roger Proksch, President and co-founder of Asylum Research. “Some other nanomechanical imaging techniques only measure the elastic modulus of materials and have no capability to measure the loss modulus. However, both the elastic and dissipative response is critical to the performance of many modern materials. Contact Resonance Viscoelastic Mapping Mode provides a more complete picture which should enable more accurate and more useful insights into how nanomechanical properties influence real-world applications of these materials.”
A number of exclusive Asylum Research technologies enable the superior performance of Contact Resonance Viscoelastic Mapping Mode. Highly damped cantilever and sample actuators were developed for both the MFP-3D and Cypher AFMs to provide exceptionally clean, wideband excitation that makes operation far more robust and accurate. Dual AC Resonance Tracking (DART) and Band Excitation electronics make it possible to rapidly measure both the contact resonance frequency and quality factor, providing measures of both the elastic and viscous responses at higher speeds. Finally, exclusive software enables users to select the most appropriate analysis models and easily guides them through the steps required to calibrate the technique. The contact resonance packages are available for both new MFP-3D and Cypher S AFM systems and as upgrades to existing systems.