Silver-filled adhesive film enables high-temperature operation
April 21, 2014 Source:
The Advanced Circuit Materials Division of Rogers Corp., Rogers, Conn., launches Coolspan thermally and electrically conductive adhesive (TECA) film, which provides reliable high temperature performance. It is a thermosetting, epoxy based, silver-filled adhesive film can bond circuit boards to heavy metal backplanes, heat sink coins, and RF module housings. The adhesive can be used as an alternative to fusion bonding, sweat soldering, or press fit metal attachment. This film provides both a thermally and electrically conductive bond interface.
Coolspan TECA film is supplied in sheet form on a PET carrier and is easy to handle when converting into preforms and when peeling from the carrier. It is able to survive lead-free solder processing and offers outstanding chemical resistance and high temperature performance, helping you to keep things cool.
It has been demonstrated to easily survive 5X lead-free solder exposures, 1000 hours at 85C/85%RH, and 190C for ten days
The Advanced Circuit Materials Division of Rogers Corp., Rogers, Conn., launches Coolspan thermally and electrically conductive adhesive (TECA) film, which provides reliable high temperature performance. It is a thermosetting, epoxy based, silver-filled adhesive film can bond circuit boards to heavy metal backplanes, heat sink coins, and RF module housings. The adhesive can be used as an alternative to fusion bonding, sweat soldering, or press fit metal attachment. This film provides both a thermally and electrically conductive bond interface.
Coolspan TECA film is supplied in sheet form on a PET carrier and is easy to handle when converting into preforms and when peeling from the carrier. It is able to survive lead-free solder processing and offers outstanding chemical resistance and high temperature performance, helping you to keep things cool.
It has been demonstrated to easily survive 5X lead-free solder exposures, 1000 hours at 85C/85%RH, and 190C for ten days