III-V metal-oxide semiconductor FET performance exceeds silicon
June 23, 2014 Source: ASM International
Researchers from the University of California, Santa Barbara (UCSB), report that they have developed the highest-performing III-V metal-oxide semiconductor (MOS) field-effect transistors. The UCSB team’s III-V MOSFETs, for the first time in the industry, exhibit on-current, off-current, and operating voltage comparable to or exceeding production silicon devices — while being constructed at small dimensions relevant to the VLSI (very-large-scale integration) industry.
For the past decade, III-V MOSFETs have been widely studied by a large number of research groups, but no research group had reported a III-V MOSFET with a performance equal to, let alone surpassing, that of a silicon MOSFET of similar size. In particular, UCSB’s transistors possess 25nm gate lengths, an on-current of 0.5mA, and off-current of 100nA per micron of transistor width, and require only 0.5 volt to operate.
“The goal in developing new transistors is to reach or beat performance goals while making the transistor smaller—it is no good getting high performance in a big transistor,” said Mark Rodwell, professor of Electrical and Computer Engineering, UCSB. “In time, the UCSB III-V MOSFET should perform significantly better than silicon FinFETs of equal size.”
The UCSB research promises to help deliver higher semiconductor performance at lower power consumption levels for next-generation, high-performance servers. The research is supported by the Semiconductor Research Corporation (SRC), the world’s leading university-research consortium for semiconductors and related technologies.
To reach this breakthrough in performance, the UCSB team made three key improvements to the III-V MOSFET structure. First, the transistors use extremely thin semiconductor channels, some 2.5nm (17 atoms) thick, with the semiconductor being indium arsenide (InAs). Making such thin layers improves the on-current and reduces the off-current. These ultra-thin layers were developed by UCSB Ph.D student Cheng-Ying Huang under the guidance of Professor Arthur Gossard.
http://semimd.com/blog/2014/06/10/research-alert-june-10-2014/