Nanodiamond-containing polymers conduct heat, resist wear
December 12, 2015 Source:
Carbodeon, Finland, has been granted a U.S. patent for detonation-synthesized diamond particles (nanodiamonds) that are combined with polymers to produce wear-resistant materials with good thermal conductivity. Potential applications include personal electronics, LED lighting, automotive applications, and machine tools.
Diamonds are the hardest natural mineral, and also one of the most thermally conductive materials known, so when nanodiamonds are mixed with thermoplastic polymers in controlled amounts, they can enable plastic materials to conduct heat at pre-determined rates, and/or to be highly wear-resistant.
Nanodiamond-impregnated polymers can deliver heat-conducting benefits for products including LED lighting, mobile devices including cellphones, and Internet-of-Things (IoT) enabled devices of any type. The hard-wearing properties mean they can also be used in the aerospace and automotive sectors to enable longer product life in hard-wear environments.
Carbodeon has been granted U.S. patent number 9085723 on their developed nanodiamond-containing thermoplastic thermal composites. The patent was filed after Carbodeon's own developments during 2012-2013, when engineers discovered that thermal conductivity of thermoplastics can be significantly enhanced by adding nanodiamonds, usually in relatively small quantities. Since filing the patent, they have continued research and are developing a range of commercial applications of the technology.
The granting of this patent represents a key part of our nanodiamond composite material portfolio. The combined coverage of our filed and granted patents will secure our position and that of our customers in several nanodiamond applications including polymers for thermal management applications, wear and corrosion resistant nanodiamond metal finishing, and wear resistant/ low friction nanodiamond fluoropolymer coatings.
Carbodeon, Finland, has been granted a U.S. patent for detonation-synthesized diamond particles (nanodiamonds) that are combined with polymers to produce wear-resistant materials with good thermal conductivity. Potential applications include personal electronics, LED lighting, automotive applications, and machine tools.
Diamonds are the hardest natural mineral, and also one of the most thermally conductive materials known, so when nanodiamonds are mixed with thermoplastic polymers in controlled amounts, they can enable plastic materials to conduct heat at pre-determined rates, and/or to be highly wear-resistant.
Nanodiamond-impregnated polymers can deliver heat-conducting benefits for products including LED lighting, mobile devices including cellphones, and Internet-of-Things (IoT) enabled devices of any type. The hard-wearing properties mean they can also be used in the aerospace and automotive sectors to enable longer product life in hard-wear environments.
Carbodeon has been granted U.S. patent number 9085723 on their developed nanodiamond-containing thermoplastic thermal composites. The patent was filed after Carbodeon’s own developments during 2012-2013, when engineers discovered that thermal conductivity of thermoplastics can be significantly enhanced by adding nanodiamonds, usually in relatively small quantities. Since filing the patent, they have continued research and are developing a range of commercial applications of the technology.
The granting of this patent represents a key part of our nanodiamond composite material portfolio. The combined coverage of our filed and granted patents will secure our position and that of our customers in several nanodiamond applications including polymers for thermal management applications, wear and corrosion resistant nanodiamond metal finishing, and wear resistant/ low friction nanodiamond fluoropolymer coatings.