Extreme selectivity etch tool enables atomic-level precision for 3D logic chips
July 1, 2016 Source:
Applied Materials Inc., Santa Clara, Calif., introduces its Applied Producer Selectra System, the industry's first extreme selectivity etch tool that presents new materials engineering capabilities for continued scaling of 3D logic and memory chips.
"One of the most significant hurdles in producing advanced chips is to selectively remove a specific material without damaging other exposed materials in the multi-layer device," says Dr. Shankar Venkataraman, vice president and general manager of Applied's Selective Removal Products Business Unit. "The Selectra system is the latest innovation in our etch portfolio of differentiated products, and creates new market opportunities by delivering the extreme selectivity required to advance Moore's Law."
Advanced microchips featuring increasingly complex structures and deep, narrow trenches are creating new manufacturing challenges. One of these challenges is the inability of wet chemistry to penetrate tiny structures; another is the removal of unwanted materials without causing damage. The Selectra system's breakthrough process accesses the smallest spaces, delivering unprecedented materials selectivity and atomic-level etch precision for a wide variety of dielectric, metal, and semiconductor films.
The system has an extensive range of processes, including the ability to achieve precisely controlled residue-free and damage-free materials removal. The system targets an expanding number of crucial etch applications for patterning, logic, foundry, 3D NAND, and DRAM. The system's versatility allows chipmakers to manufacture leading-edge 3D devices and to explore new architectures, materials, and integration options.
Selectra systems are in volume production at foundry, logic, and memory chipmakers, and demand is gaining momentum as customers begin to manufacture their most advanced device designs.
Applied Materials is the leader in materials engineering solutions used to produce virtually every new chip and advanced display in the world. Its expertise in modifying materials at atomic levels and on an industrial scale enables customers to transform possibilities into reality.
Applied Materials Inc., Santa Clara, Calif., introduces its Applied Producer Selectra System, the industry’s first extreme selectivity etch tool that presents new materials engineering capabilities for continued scaling of 3D logic and memory chips.
“One of the most significant hurdles in producing advanced chips is to selectively remove a specific material without damaging other exposed materials in the multi-layer device,” says Dr. Shankar Venkataraman, vice president and general manager of Applied’s Selective Removal Products Business Unit. “The Selectra system is the latest innovation in our etch portfolio of differentiated products, and creates new market opportunities by delivering the extreme selectivity required to advance Moore’s Law.”
Advanced microchips featuring increasingly complex structures and deep, narrow trenches are creating new manufacturing challenges. One of these challenges is the inability of wet chemistry to penetrate tiny structures; another is the removal of unwanted materials without causing damage. The Selectra system’s breakthrough process accesses the smallest spaces, delivering unprecedented materials selectivity and atomic-level etch precision for a wide variety of dielectric, metal, and semiconductor films.
The system has an extensive range of processes, including the ability to achieve precisely controlled residue-free and damage-free materials removal. The system targets an expanding number of crucial etch applications for patterning, logic, foundry, 3D NAND, and DRAM. The system’s versatility allows chipmakers to manufacture leading-edge 3D devices and to explore new architectures, materials, and integration options.
Selectra systems are in volume production at foundry, logic, and memory chipmakers, and demand is gaining momentum as customers begin to manufacture their most advanced device designs.
Applied Materials is the leader in materials engineering solutions used to produce virtually every new chip and advanced display in the world. Its expertise in modifying materials at atomic levels and on an industrial scale enables customers to transform possibilities into reality.