Third quarter silicon wafer shipments set new record of 3,255 million square inches
November 18, 2018 Source:
The SEMI Silicon Manufacturers Group (SMG), Milpitas, Calif., reports that worldwide silicon wafer area shipments increased during the third quarter 2018, surpassing record second quarter 2018 area shipments to set another all-time high.
Total silicon wafer area shipments reached 3,255 million square inches during the most recent quarter, a 3.0 percent rise from the 3,164 million square inches shipped during the previous quarter. New quarterly total area shipments clocked in 8.6 percent higher than third quarter 2017 shipments.
“Silicon shipment volumes remained at record levels during the third quarter,†said Neil Weaver, chairman SEMI SMG and Director, Product Development and Applications Engineering of Shin Etsu Handotai America. “Silicon shipments are mirroring this year’s strong semiconductor unit growth in support of a growing and diversified electronics market during our stable economy.â€
Silicon wafers are the fundamental building material for semiconductors, which in turn, are vital components of virtually all electronics goods, including computers, telecommunications products, and consumer electronics. The highly engineered thin round disks are produced in various diameters (from one inch to 12 inches) and serve as the substrate material on which most semiconductor devices, or chips, are fabricated.
All data cited in this release is inclusive of polished silicon wafers, including virgin test wafers and epitaxial silicon wafers, as well as non-polished silicon wafers shipped by the wafer manufacturers to the end-users.
The Silicon Manufacturing Group (SMG) is a sub-committee of the SEMI Electronic Materials Group (EMG) and is open to SEMI members involved in manufacturing polycrystalline silicon, monocrystalline silicon or silicon wafers (e.g., as cut, polished, epi, etc.). The purpose of the group is to facilitate collective efforts on issues related to the silicon industry including the development of market information and statistics about the silicon industry and the semiconductor market.
The SEMI Silicon Manufacturers Group (SMG), Milpitas, Calif., reports that worldwide silicon wafer area shipments increased during the third quarter 2018, surpassing record second quarter 2018 area shipments to set another all-time high.
Total silicon wafer area shipments reached 3,255 million square inches during the most recent quarter, a 3.0 percent rise from the 3,164 million square inches shipped during the previous quarter. New quarterly total area shipments clocked in 8.6 percent higher than third quarter 2017 shipments.
“Silicon shipment volumes remained at record levels during the third quarter,” said Neil Weaver, chairman SEMI SMG and Director, Product Development and Applications Engineering of Shin Etsu Handotai America. “Silicon shipments are mirroring this year’s strong semiconductor unit growth in support of a growing and diversified electronics market during our stable economy.”
Silicon wafers are the fundamental building material for semiconductors, which in turn, are vital components of virtually all electronics goods, including computers, telecommunications products, and consumer electronics. The highly engineered thin round disks are produced in various diameters (from one inch to 12 inches) and serve as the substrate material on which most semiconductor devices, or chips, are fabricated.
All data cited in this release is inclusive of polished silicon wafers, including virgin test wafers and epitaxial silicon wafers, as well as non-polished silicon wafers shipped by the wafer manufacturers to the end-users.
The Silicon Manufacturing Group (SMG) is a sub-committee of the SEMI Electronic Materials Group (EMG) and is open to SEMI members involved in manufacturing polycrystalline silicon, monocrystalline silicon or silicon wafers (e.g., as cut, polished, epi, etc.). The purpose of the group is to facilitate collective efforts on issues related to the silicon industry including the development of market information and statistics about the silicon industry and the semiconductor market.