Bruker D8 Discover Plus X-ray diffraction instrument features highly parallel X-ray beam
September 20, 2019 Source:
Bruker Corp., Billerica, Mass., has released the D8 Discover Plus x-ray diffraction (XRD) solutions, featuring the new non-coplanar arm and the Montel Plus x-ray optics. The non-coplanar arm allows the instrument to perform in-plane diffraction measurements with unparalleled accuracy and ease-of-use. In combination with the patented Automated Torque Control technology of the Atlas goniometer, the non-coplanar arm sets a new benchmark for in-plane diffraction.
For successful in-plane diffraction on ultra-thin layers, the key to success is a highly parallel and intense x-ray beam, which is provided by the unique Bruker IμS x-ray source with the new Montel Plus optics. The D8 Discover Plus with the non-coplanar arm and Montel Plus optics increases measured intensities by up to one order of magnitude, resulting in best data quality for new insights into structural properties.
The D8 Discover Plus also comes with the latest x-ray detector technology, including LynxEye XE-T, the strip detector with the highest available energy resolution; or the multi-mode Hybrid Photon Counting (HPC) detector Eiger2 R 500K, both offering unmatched capabilities for various analytical tasks in materials research.
The D8 Discover Plus offers compatibility with other D8 family components. It features Diffrac.Davinci for real-time component recognition, as well as Diffrac.Snap-lock for alignment-free exchange of system subunits without tools.
Bruker Corp., Billerica, Mass., has released the D8 Discover Plus x-ray diffraction (XRD) solutions, featuring the new non-coplanar arm and the Montel Plus x-ray optics. The non-coplanar arm allows the instrument to perform in-plane diffraction measurements with unparalleled accuracy and ease-of-use. In combination with the patented Automated Torque Control technology of the Atlas goniometer, the non-coplanar arm sets a new benchmark for in-plane diffraction.
For successful in-plane diffraction on ultra-thin layers, the key to success is a highly parallel and intense x-ray beam, which is provided by the unique Bruker I?S x-ray source with the new Montel Plus optics. The D8 Discover Plus with the non-coplanar arm and Montel Plus optics increases measured intensities by up to one order of magnitude, resulting in best data quality for new insights into structural properties.
The D8 Discover Plus also comes with the latest x-ray detector technology, including LynxEye XE-T, the strip detector with the highest available energy resolution; or the multi-mode Hybrid Photon Counting (HPC) detector Eiger2 R 500K, both offering unmatched capabilities for various analytical tasks in materials research.
The D8 Discover Plus offers compatibility with other D8 family components. It features Diffrac.Davinci for real-time component recognition, as well as Diffrac.Snap-lock for alignment-free exchange of system subunits without tools.