Industry News
Keep up-to-date on the latest advances in the metals and materials industry with ASM Industry News.
-
1282 items found
University of Chicago researchers develop compounds to join semiconductors
Published: February 18, 2015
Researchers at the University of Chicago have reportedly developed compounds of cadmium, lead, and bismuth that can be applied as a liquid or paste to join two semiconductors or semiconductor pieces by heating them to several hundred degrees Celsius.
News, Magazine & Media / Industry News
Optomec partners with Ceradrop to expand printed electronics
Published: February 09, 2015
Optomec, Albuquerque, N.M., has signed an agreement with Ceradrop to be its exclusive representative in France for Aerosol Jet systems used for printing electronics.
News, Magazine & Media / Industry News
New specimen preparation solution
Published: February 06, 2015
EXpressLO LLC, Lehigh Acres, Fla., released the Aspirato lift out module for the EXpressLO ex situ lift out station.
News, Magazine & Media / Industry News
Femtosecond lasers make metals superhydrophobic
Published: January 25, 2015
Scientists at the University of Rochester, N.Y., have reportedly transformed platinum, titanium, and brass into superhydrophobic materials with femtosecond laser pulses.
News, Magazine & Media / Industry News
Craic adds Raman microspectroscopy to its microspectrophotometer
Published: January 19, 2015
Craic Technologies, San Dimas, Calif., has added Raman microspectroscopy to its flagship product, the 20/30 Perfect Vision microspectrophotometer.
News, Magazine & Media / Industry News
Oxford Instruments Asylum Research Announces AFM Image Contest Winners
Published: January 19, 2015
Oxford Instruments Asylum Research, Santa Barbara, Calif., announces the winners of its AFM Image Contest.
News, Magazine & Media / Industry News
JEOL and UC Irvine partner for electron microscopy and materials science research
Published: January 19, 2015
JEOL USA, Peabody, Mass., and the University of California's Irvine Materials Research Institute (IMRI) have entered into a strategic partnership to create a premier electron microscopy and materials science research facility.
News, Magazine & Media / Industry News
Shimadzu spectrophotometer with three detectors provides high-resolution analyses
Published: January 19, 2015
Shimadzu, Japan, introduces its new UV-3600 Plus UV-VIS-NIR spectrophotometer, which is equipped with three detectors: a photomultiplier tube for ultraviolet and visible regions, and InGaAs and cooled PbS detectors for the near-infrared region.
News, Magazine & Media / Industry News
Magnonic holographic memory chosen as one of “Ten Breakthroughs of the Year”
Published: January 19, 2015
Physics World, the magazine of the Institute of Physics, U.K., has selected Magnonic Holographic Memory as one of the "2014 Ten Breakthroughs of the Year."
News, Magazine & Media / Industry News
Brewer Science wins award from SEMI for anti-reflective coatings in optical lithography
Published: January 19, 2015
Brewer Science Inc., San Jose, Calif., was honored as the recipient of the 2014 SEMI award for North America for his impact on the manufacturing of integrated circuits in the semiconductor industry.
News, Magazine & Media / Industry News