Record efficiency of 68.9% for GaAs thin film photovoltaic cell under laser light
Published: July 18, 2021
The research team at Fraunhofer ISE, Germany, achieved a record conversion efficiency of 68.9% under monochromatic laser light with a new thin film photovoltaic cell based on gallium arsenide.
News, Magazine & Media / Industry News
New method to improve durability of nano-electronic components
Published: July 18, 2021
Researchers at University of South Florida, Tampa, Fla., developed a novel approach to mitigating electromigration in nanoscale electronic interconnects, ubiquitous in state-of-the-art integrated circuits.
News, Magazine & Media / Industry News
Ted Pella acquires the assets of LatticeGear
Published: July 18, 2021
LatticeGear LLC, Hillsboro, Ore., has sold their product, manufacturing, and associated assets to Ted Pella Inc. of Redding, Calif.
News, Magazine & Media / Industry News
WITec GmbH joins Oxford Instruments plc
Published: July 18, 2021
Oxford Instruments plc, United Kingdom, announced the acquisition of WITec Wissenschaftliche Instrumente und Technologie GmbH, Germany, a leading provider of Raman microscopy imaging solutions, for a cash-free, debt-free consideration of €42m, of which €5m is conditional on trading performance over a period of 12 months following completion.
News, Magazine & Media / Industry News
Microscope uncovers secrets of a material’s structure
Published: July 01, 2021
Scientists at École Polytechnique Fédérale de Lausanne (EPFL) in Switzerland have made an important discovery about the structure of barium titanate, a material used in everyday objects. Their findings refute existing theories on the displacement of the material’s atoms.
News, Magazine & Media / Industry News
Robust federal incentives for domestic chip manufacturing would create an average of nearly 200,000 American jobs annually as fabs are built adding nearly $25 Billion annually to U.S. economy
Published: June 21, 2021
The Semiconductor Industry Association, Washington, in partnership with Oxford Economics, England, released a study analyzing the semiconductor workforce in the United States and the economic benefits that would come from robust federal investment in domestic chip production.
News, Magazine & Media / Industry News
Bosch opens $1.2B semiconductor factory in eastern Germany
Published: June 20, 2021
Bosch, Germany, opened a 1 billion euro ($1.2 billion) chip factory in the eastern city of Dresden to help meet the growing demand for semiconductors.
News, Magazine & Media / Industry News
Researchers tame silicon to interact with light for next-generation microelectronics
Published: June 20, 2021
Skoltech researchers and their colleagues from RAS Institute for Physics of Microstructures, Lobachevsky State University of Nizhny Novgorod, ITMO University, Lomonosov Moscow State University, and A.M. Prokhorov General Physics Institute, Russia, have found a way to increase photoluminescence in silicon, the notoriously poor emitter and absorber of photons at the heart of all modern electronics.
News, Magazine & Media / Industry News
Engineers create a programmable fiber
Published: June 20, 2021
Researchers at Massachusetts Institute of Technology, Cambridge, have created the first fiber with digital capabilities, able to sense, store, analyze, and infer activity after being sewn into a shirt.
News, Magazine & Media / Industry News
Unveiling what governs crystal growth
Published: June 20, 2021
Scientists from the U.S. Department of Energy’s Argonne National Laboratory, Lemont, Ill., along with three universities, have revealed new insights into the mechanism behind how gallium nitride crystals grow at the atomic scale.
News, Magazine & Media / Industry News