Penn State research lays groundwork for ultra-thin, energy efficient photodetector on glass
November 12, 2020 Source: ASM International
Researchers at Penn State, University Park, Pa., published a new paper in ACS Nano integrating photodetectors with durable Gorilla glass, the material used for smart phone screens manufactured by Corning Incorporated.
Integrating photodetectors with Gorilla glass could lead to the commercial development of “smart glass,” or glass equipped with automatic sensing properties. Smart glass has a number of applications ranging from imaging to advanced robotics, according to the researchers.
“There are two problems to address when attempting to manufacture and scale photodetectors on glass,” said principal investigator Saptarshi Das, assistant professor of engineering science and mechanics (ESM). “It must be done using relatively low temperatures, as the glass degrades at high temperatures, and must ensure the photodetector can operate on glass using minimal energy.”
To overcome the first challenge, Das, along with ESM doctoral student Joseph R. Nasr, determined that the chemical compound molybdenum disulfide was the best material to use as a coating on the glass.
Joshua Robinson, professor of materials science and engineering (MatSE) and MatSE doctoral student Nicholas Simonson used a chemical reactor at 600°C—a low enough temperature so as not to degrade the Gorilla glass—to fuse together the compound and glass. They then turned the glass and coating into a photodetector by patterning it using a conventional electron beam lithography tool.
“We then tested the glass using green LED lighting, which mimics a more natural lighting source unlike laser lighting, which is commonly used in similar optoelectronics research,” Nasr said.
The ultra-thin body of the molybdenum disulfide photodetectors allows for better electrostatic control, and ensures it can operate with low power—a critical need for the smart glass technology of the future.
If developed commercially, smart glass could lead to technology advances in wide-ranging sectors of industry including in manufacturing, civil infrastructure, energy, health care, transportation and aerospace engineering, according to the researchers. The technology could be applied in biomedical imaging, security surveillance, environmental sensing, optical communication, night vision, motion detection, and collision avoidance systems for autonomous vehicles and robots.
“Smart glass on car windshields could adapt to oncoming high-beam headlights when driving at night by automatically shifting its opacity using the technology,” Robinson said. “And new Boeing 757 planes could utilize the glass on their windows for pilots and passengers to automatically dim sunlight.”
Image – This graphic depicts molybdenum disulfide growth on Gorilla glass, the process that turns normal glass into a photodetector. Courtesy of Jennifer M. McMann / Penn State Materials Research Institute.
For more information:
Pennsylvania State University
https://www.psu.edu/
Subject Classifications
Aerospace and Defense
Automobiles and Ground Transportation
Consumer Products
Electronics
news
News Articles
Uncategorized