Imaging technique reveals strains and defects in vanadium oxide
October 22, 2021 Source: ASM International
Researchers at Rensselaer Polytechnic Institute, Troy, N.Y., have developed a new technique based on coherent X-ray diffraction imaging for revealing defects in nanostructured vanadium oxide, a widely used transition metal with many potential applications including electrochemical anodes, optical applications, and supercapacitors. In the research, published in the Royal Chemical Society journal CrystEngComm, the team detailed a lensless microscopy technique to capture individual defects embedded in vanadium oxide nanoflakes.
“These observations could help explain the origin of defects in structure, crystallinity, or composition gradients observed near grain boundaries in other thin-film or flake technologies,” said Edwin Fohtung, an expert in novel synchrotron scattering and imaging techniques and associate professor of materials science and engineering at RPI leading the research. “We believe that our work has the potential to change how we view the growth and non-destructive three-dimensional imaging of nanomaterials.”
Vanadium oxide is currently used in many technological fields such as energy storage, and can also be used in constructing field-effect transistors owing to metal insulating transition behavior that can be adjusted with an electric field. However, strain and defects in the material can alter its functionality, creating the need for non-destructive techniques to detect those potential flaws.
The new technique relies on a type of circular particle accelerator known as a synchrotron. Synchrotrons work by accelerating electrons through sequences of magnets until they reach almost the speed of light. These fast-moving electrons produce very bright intense light, predominantly in the X-ray region. This synchrotron light, as it is named, is millions of times brighter than light produced from conventional sources and 10 billion times brighter than the sun.
The group successfully used this light to develop techniques and capture minute matter such as atoms and molecules and now defects. When used to probe crystalline materials, this technique is known as Bragg coherent diffraction imaging (BCDI). In their research, the team used a BCDI approach to reveal nanoscale properties of electron densities in crystals, including strain and lattice defects.
Image – Courtesy of: Rensselaer Polytechnic Institute
For more information:
Rensselaer Polytechnic Institute
https://www.rpi.edu/
Subject Classifications
Materials Properties and Performance
Materials Testing and Evaluation
news
News Articles
Uncategorized