How long can fiber-reinforced polymer sustain concrete structures? Scientists answer
November 15, 2021 Source: ASM International
In modern society, the majority of our infrastructure (buildings, bridges, tunnels, etc.) is made of aging concrete. A recently developed cost-effective method of sustaining this infrastructure involves an external coating with fiber-reinforced polymer (FRP) composites. But is this a temporary patch or a durable solution?
A 13-year-long study at the National Korea Maritime and Ocean University, Korea, published in Composites Part B finally answers this question, taking us one step closer to its widespread utilization.
In the FRP-strengthening of concrete, glass or carbon fiber–reinforced polymer (GFRP or CFRP) composites are bonded onto concrete using an epoxy adhesive. These sheets provide additional support and strengthen the concrete by protecting them from harsh environmental conditions, such as high moisture levels and temperatures. But these same environmental conditions can potentially degrade the concrete-FRP bond as well, causing the FRP protection system to fail prematurely.
Prof. Jaeha Lee from Korea Maritime and Ocean University, a lead researcher in the study, says, “The information available on FRP-concrete bond behavior following sustained loads in different environments is very limited, particularly for periods beyond two years.”
The researchers tested both CFRP and GFRP systems under various indoor and outdoor environmental conditions for changes in a parameter called the debond onset strain. This is a measure of the deformation that occurs before failure; larger strains usually forewarn imminent failure.
The researchers found that environmental conditions had a significant impact on bond behavior. At the end of 13 years, larger reductions in debond strains were observed in outdoor beams than indoor beams. Further, the bond behavior varied between materials: changes in debond strain were negligible in indoor CFRP beams, while in outdoor GFRP beams, there was a notable decrease.
Prof. Lee stresses the importance of such tests for future use, stating: “If the long-term durability of concrete-FRP interfaces is evaluated, the use of this strengthening system is expected to increase with minimum investment. This will be great for affordably maintaining a safer city by minimizing the risk of collapse or damage of existing structures.”
Image – Fiber reinforced polymer coatings are an affordable way to externally strengthen concrete structures, but how long does the protection last? Scientists find out. Courtesy of: Korea Maritime and Ocean University
More information:
National Korea Maritime and Ocean University
https://www.kmou.ac.kr/english/main.do
Subject Classifications
Buildings and Infrastructure
Industries and Applications
Materials Properties and Performance
Materials Testing and Evaluation
news
News Articles
Uncategorized