New cathode design solves major barrier to better lithium-ion batteries
September 15, 2022 Source: ASM International
Researchers at the U.S. Department of Energy’s (DOE) Argonne National Laboratory, Lemont, Ill., made another breakthrough with the NMC cathode, finding a boundary-free electrode structure eliminates reactions that diminish battery life.
Argonne researchers have a long history of breakthrough discoveries with lithium-ion batteries. Many of these discoveries have focused on a battery cathode known as NMC, a nickel-manganese-cobalt oxide. Batteries with this cathode now power the Chevy Bolt.
The team’s new structure for the cathode’s micro-sized particles could lead to longer-lasting and safer batteries able to operate at very high voltage and power vehicles for longer driving ranges.
Present-day NMC cathodes have posed a major barrier to operation at high voltage. With charge-discharge cycling, performance rapidly declines due to cracks forming in the cathode particles. For several decades, battery researchers have been seeking ways to eliminate these cracks.
One past approach involved microscale spherical particles consisting of numerous much smaller particles. The large spherical particles are polycrystalline, with differently oriented crystalline regions, resulting in grain boundaries between particles, which cause cracking upon battery cycling. To prevent this, Argonne researchers had previously developed a protective polymer coating around each particle. This coating surrounds the large spherical particles and smaller ones inside them.
A different approach to avoid this cracking involves single-crystal particles. Electron microscopy of these particles indicated they have no boundaries. But, cathodes made from both coated polycrystals and single crystals still formed cracks with cycling.
Extensive X-ray analyses of the cathodes performed at the Advanced Photon Source (APS) and Center for Nanoscale Materials (CNM), DOE Office of Science user facilities at Argonne using five APS beamlines (11-BM, 20-BM, 2-ID-D, 11-ID-C and 34-ID-E) revealed that what scientists had believed were single crystals, as evidenced by electron and X-ray microscopy, actually had boundaries inside. Scanning and transmission electron microscopies at CNM verified the finding.
“When we look at the surface morphology of these particles, they look like single crystals,” said physicist Wenjun Liu at Argonne. “But when we use a technique called synchrotron x-ray diffraction microscopy and other techniques at the APS, we find boundaries hiding inside.”
The team developed a method for producing boundary-free single crystals. Testing small cells with these single-crystal cathodes at very high voltage showed a 25% increase in energy storage per unit volume, with almost no loss of performance over 100 cycles of testing. By contrast, over the same cycle life, the capacity declined by 60% to 88% in NMC cathodes composed of single crystals with many internal boundaries or with coated polycrystals.
Calculations at the atomic scale revealed the mechanism behind the capacity decline in the cathode. According to nanoscientist Maria Chan in CNM, compared to the regions away from them, boundaries are more vulnerable towards the loss of oxygen atoms when the battery is being charged. This oxygen loss leads to degradation with cell cycling. “Our calculations showed how boundaries lead to oxygen release at high voltage and, therefore, performance decline,” Chan said.
Eliminating the boundaries prevents oxygen release and thereby improves the cathode safety and stability with cycling. Oxygen release measurements at APS and the Advanced Light Source at DOE’s Lawrence Berkeley National Laboratory supported this finding.
“We now have guidelines that battery manufacturers can use to prepare cathode material that is boundary free and works at high voltage,” said Khalil Amine, an Argonne Distinguished Fellow. “And the guidelines should apply to other cathode materials besides NMC.”
A paper on this research appeared in Nature Energy.
Image – Boundaries within cathode materials are undesirable because they lead to performance degradation. Courtesy of: Maria Chan/Argonne National Laboratory.
For more information:
Argonne National Laboratory
https://www.uchicagoargonnellc.org/
Subject Classifications
Batteries and Energy Storage
Industries and Applications
Materials Testing and Evaluation
news
News Articles
Phase Diagrams and Crystallography
Uncategorized