Oxford Instruments validates contactless SiC plasma epi-prep on power devices with technology acceleration partner Clas-SiC
September 15, 2022 Source: ASM International
Recently Oxford Instruments, UK, announced the launch of their SiC substrate contactless plasma polishing solution. The aim of this technology is to supersede the established chemical mechanical planarization CMP process, with a clean, dry, lower cost, higher yield and sustainable alternative. The project has taken a big step forward by collaborating with Clas-SiC and qualifying whole wafer 1200 V MOSFET devices, further boosting confidence in the new solution and its impact on SiC power semiconductor devices.
“The 1200 V MOSFET parametric results and yield are very encouraging, being very comparable to those of conventionally CMP prepared wafers which were used as a direct comparison. We rely on multiple vendors for substrates due to supply limitations, so incoming material variability is a challenge across the device manufacture industry. The fact that substrates were sourced, processed at Oxford Instruments, incorporated into our production flow on two separate device types and achieved such comparable results so soon, should give Oxford Instruments confidence that their process window is robust and fit for purpose.
For a first result this is a hugely positive outcome and gives confidence that Oxford Instrument’s new technology has a great future in reducing the cost of the very expensive incoming SiC substrates. This will be very important in reducing the cost of SiC based power converters and in increasing their adoption in the marketplace,” said David Clark, Technology & Customer Relations manager, Clas-SiC.
Demand currently exceeds supply for SiC substrates, and the wide band gap semiconductors that are manufactured on the substrates are also in short supply. This production gap is set to exponentially increase, as high-growth electric vehicle and sustainable energy markets incorporate ever increasing amounts of these compound semiconductors into their applications, so new solutions are therefore needed.
Plasma polishing is a plug and play alternative to CMP, that straightaway reduces the cost per wafer with reduced OPEX, but is also a key enabling technology to accelerate the transition to thinner slices and more wafers per boule at 150mm and 200mm. This, and other innovative SiC technologies, has the potential to shift the production paradigm so SiC supply chains can comfortably support high-growth technology markets in a sustainable way.
Image: PlasmaPro 100 Cobra ICP.
For more information:
Oxford Instruments Plasma Technology