Samco unveils plasma-enhanced ALD system for SiC and GaN power devices
October 21, 2022 Source: ASM International
Samco, Japan, a leading manufacturer of etching, deposition, and surface treatment processing equipment for the semiconductor and related industries and academic facilities, launches the new AD-800LP Plasma Enhanced Atomic Layer Deposition (PEALD) system. The main target of the system is gate oxide film deposition for next-generation power devices of silicon carbide (SiC) and gallium nitride (GaN) materials, which will play important role toward carbon neutral.
The AD-800LP plasma enhanced ALD system is a multi-purpose R&D system equipped with a unique ICP plasma source called Tornado ICP, in addition to the conventional thermal ALD capability. AD-800LP enables various film deposition such as oxide or nitride films by Tornado ICP, which is Samco’s proprietary plasma technology and is different from remote plasma. Tornado ICP enables stable plasma discharge even in the high-pressure range during ALD deposition.
“We are also considering a cluster ALD system that can connect multiple reaction chambers for production” says Tsukasa Kawabe, President and COO of Samco. “The launch of the AD-800LP will greatly enhance our presence in the world ALD equipment market,” he says.
As a global mid-sized company, Samco has successfully delivered numerous dry etch systems and plasma enhanced CVD systems for the electronic device field, mainly for compound semiconductors such as SiC, GaN, and GaAs, not only in Japan but also in the United States, Europe, Taiwan, Korea, China, Southeast Asia, India, and other countries.
Image – Samco’s AD-800LP system.
For more information:
Samco Inc.