Skip to content
Heat Treating Society
Become a Member
  • Membership
    • About Us
    • Join/Renew HTS Today!
    • Membership & Benefits
    • Society Board
    • Society Awards
    • Get Involved
      • Committees: Get Involved
      • HTS Board Nominations
  • Material Resources
    • ASM Handbooks
    • Technical Books
    • Journal of Materials Engineering and Performance
    • Heat Treater’s Guide
    • HTS Buyer’s Guide
  • Education
    • Certificate Program
    • Heat Treat Courses
  • Events
    • View All Upcoming Events
    • Heat Treat Mexico 2026
    • IMAT 2026
  • Industry News

Cleveland-Cliffs Inc. acquires Arcelor Mittal USA for its automotive and other markets

Cleveland Cliffs Inc. announces that it has entered into a definitive agreement with ArcelorMittal S.A., in which Cleveland-Cliffs will acquire substantially all of the operations of ArcelorMittal USA LLC and its subsidiaries for approximately $1.4 billion.

Continue reading

Instron offers free online course titled Basic Introduction to Materials Testing

Instron, Norwood, Mass., announces that it will continue to offer free access to its Introduction to Materials Testing course to all students and professors (English only).

Continue reading

RSP Technology’s rapid solidification process produces strong nano-grained aluminum

RSP Technology, The Netherlands, announces that it has developed a superfast aluminum melt-spinning process that produces billets with an almost nano-grained crystalline structure that can be machined like conventional aluminum, but resulting parts will be as strong as titanium.

Continue reading

Seco Warwick Super IQ hybrid heat treating system installed at Rex Heat Treat

Seco Warwick, Meadville, Pa., announces that its Super IQ hybrid heat treating system, which combines a conventional and vacuum system, has achieved its first commercial deployment.

Continue reading

One Minute Mentor: Influence of Forging and Finish Temperatures

The temperature of a thermomechanical treatment affects grain size via the transformation of recrystallized austenite and its subsequent transformation to ferrite and pearlite.

Continue reading

Ipsen reports five vacuum furnace orders during July from various industries

Ipsen, Cherry Valley, Ill., announces that despite uncertain market conditions presented by the Coronavirus pandemic, the company saw an increase in orders placed during July, building positive momentum for the third quarter.

Continue reading

Solar Atmospheres Mentor all-metal vacuum furnace processes superalloys and titanium

Solar Atmospheres, Souderton, Pa., recently installed another all-metal hot zone vacuum furnace at its Clearview Road facility in Souderton.

Continue reading

American Iron and Steel Institute releases annual statistical report for 2019

The American Iron and Steel Institute (AISI), Washington, announces the release of its 2019 Annual Statistical Report, which provides comprehensive data on the U.S. steel industry and select data on the North American steel industry as a whole.

Continue reading

Heat treatment parameters optimized for reduced crack susceptibility in AM Hastelloy X

Engineers from the Edison Welding Institute, Columbus, Ohio, presented a discussion at the ASM International MS&T 2019 conference, of a study in which they reduced crack susceptibility in additively manufactured parts made of Hastelloy X.

Continue reading
HTS_logo_White-2
ASM World Headquarters
9639 Kinsman Road
Materials Park, OH 44073-0002
  • +1 440.671.3800
  • Member Service Center
Facebook-f X-twitter Linkedin Instagram Youtube
About ASM
  • Contact Us
  • About HTS
  • Advertise with Us
  • Technical Support
  • Legal
Membership
  • Join
  • Benefits
  • Board
  • Awards
Popular Subjects
Materials
  • Carbon and Alloy Steels
  • Stainless Steels
  • Aluminium
  • Titanium
  • Magnesium
Processing & Performance
  • Heat Treating
Who We Are

The ASM Heat Treating Society is the world’s premier membership society dedicated to the advancement of heat treating as a theoretical and applied discipline.

Affiliate Societies