GF Linamar wins $300 million contract for magnesium cross-car beams for pickup trucks

GF Linamar, Mills River, N.C., a joint venture between GF Automotive and Linamar, has been awarded a $300 million contract over a period of five years to produce lightweight magnesium automotive components for a U.S. manufacturer.

Nitrex Nitreg nitriding system improves fatigue resistance for automotive springs

Nitrex Metal, Montreal, has successfully installed and commissioned an NX-1230 potential-controlled Nitreg nitriding system for processing automotive springs for a customer in Korea.

Air Products to introduce intelligent atmosphere analyzers at Heat Treat 2017

Air Products, Lehigh Valley, Pa., will introduce its Intelligent Atmosphere Analyzers, enabled by the Industrial Internet of Things (IIoT), at Heat Treat 2017 in Columbus, Ohio, from October 24-26.

Lindberg MPH ships tube heat-treating furnace for research and development

Lindberg MPH, Riverside, Mich., has shipped a 2190°F hinged three-zone furnace to an R&D lab for heat treating process tubes and retorts made of ceramic, quartz, or metal alloys.

Wisconsin Oven ships heavy duty walk-in ovens to Chinese auto parts maker

Wisconsin Oven Corp., East Troy, Wis., has shipped two natural-gas direct-fired heavy-duty walk-in series ovens to a manufacturer of automotive parts in China.

Spray Tips: Fluidized Bed Powder Feeders

In fluidized-bed powder feeders, a bed of powder is continuously agitated by a fluidizing gas, in this case the carrier gas.