Message from the President: Thermal Spray Characterization Wrap-Up

It was great to see so many of you at the Thermal Spray Characterization: Materials, Coatings and Processes event held in Charleston last month. I've received a lot of very positive feedback from the attendees of this event. A big thank you again to Rick Bajan and the organizing committee which made this event possible.

Spray Tips: Coating Structures

The angle of impingement of the spray stream is a source of porosity, because of shadowing. The diagram illustrates the type of shadowing generally associated with coatings sprayed at angles below 45° from the optimal normal angle of incidence.

Retech Systems develops hybrid plasma arc melting system for titanium aluminides

Retech Systems LLC, Ukiah, Calif., reports that, after years of research and development between Retech and partner Ti-Solutions GmbH of Germany, Retech has been granted patents for a hybrid plasma-arc melting plus cold wall induction system for titanium aluminides.

Optomec and partners develop cost-effective copper inks for printed electronics

Optomec, Albuquerque, N.M., announces significant improvements in the ability to effectively print and post-process copper and copper/nickel (i.e., Constantan) inks on its Aerosol Jet systems.

Oerlikon to acquire Scoperta for its materials development via computational software

Oerlikon, Switzerland, announces that it has signed an agreement to acquire Scoperta Inc., San Diego, an innovative developer of advanced materials via computational software.

British hospital 3D prints custom medical models, reduces surgery time by hours

Stratasys, Minneapolis, announces that its PolyJet 3D printing technology is helping to improve life-changing maxillofacial surgeries at the Queen Elizabeth Hospital in Birmingham, England, by 3D printing customized models for pre-surgical preparation, thus enabling a reduction of up to 93% in surgical planning time associated with standard anatomical models.