Skip to content

Instron website explains new ISO 6892-1:2016 for ambient tensile testing of metals

Instron, Norwood, Mass., reports that the newly released ISO 6892-1:2016 standard for ambient tensile testing of metallic materials provides greater clarity of the major changes that were introduced in the previous version, ISO 6892-1:2009.

Argonne self-healing diamondlike carbon tribofilms reduce friction by 25 to 40%

Argonne National Laboratory, Lemont, Ill., announces that a research team has developed a self-lubricating diamondlike carbon tribofilm that regenerates itself by breaking down the molecules of lubricating oil and rebuilding the tribofilm as it is worn away.

Materion acquires Heraeus target materials for its semiconductor and other markets

Materion Corp., Mayfield Heights, Ohio, announces that it has acquired the target materials business of the Heraeus Group to strengthen its position in precious and non-precious target materials for the semiconductor, architectural and automotive glass, photovoltaic, and display markets.

One Minute Mentor: Nitriding in Fluidized-Bed Reactors at Low Temperatures

In nitriding treatment furnaces, the heating is done electrically, and the fluidizing gas composition is chosen to provide the optimum chemistry for the desired surface treatment (usually a mixture of NH3 + N2, with CH4 added when nitrocarburizing is desired).

Wisconsin Oven composite curing ovens feature temperature uniformity of ±5°F

Wisconsin Oven Corp., East Troy, Wis., has shipped three electrically heated, heavy-duty walk-in ovens with temperature uniformity of ±5°F for composite curing.

Seco Warwick enables constant control of temperature in multi-chamber heat-treat furnaces

Seco Warwick, Meadville, Pa., announces that its engineering team has designed an innovative technology for continuous control over the heating and cooling of the entire cycle in multi-chamber furnaces.