Skip to content

One Minute Mentor: Horizontal Retort Furnace

Gas nitriding and nitrocarburizing processes can be processed with fixed gasifying amounts of ammonia, nitrogen, and, for nitrocarburizing, a carburizing and oxidizing agent. However, this does not produce consistent results if different load surfaces are treated with the same fixed gasifying amounts. Furthermore, especially for nitriding processes, the ammonia gasifying has to be reduced or diluted with nitrogen after several hours because the nitrogen uptake of a load decreases. Another quite popular method, usually called

Solar Atmospheres of California adds Airbus approval

Solar Atmospheres, Fontana, Calif., has announced that they are now Airbus approved for heat treating. Frank Trujillo, director of Sales for Solar Atmospheres of California, stated that, “Many Airbus suppliers were in need of a heat treater in the West that could process parts, plates and bars in support of increased Airbus production rates. SCA is proud to be a partner on the Airbus Team!” With our wide range of furnaces, we are capable of

Nitrex installs nitriding system at Akademi Metalurji

Nitrex Vacuum, Quebec, has installed a turnkey nitriding system at Akademi Metalurji, a full-service commercial heat-treating solutions provider located in Turkey. The project includes a mid-sized pit-type furnace, advanced controls, three process technologies along with accelerated cooling.  The decision to invest in a new nitriding system was driven by the company’s objective to overcome efficiency and quality challenges faced with their previous furnace at the Gebze facility. The prior system consumed excessive amounts of process gases

Wisconsin Oven ships electrically heated horizontal quench system

Wisconsin Oven, East Troy, announced the shipment of an Electrically Heated Horizontal Quench System to a manufacturer of products for the automotive industry. This system will be used for the solution treatment of aluminum. The maximum temperature for this horizontal quench furnace is 1200°F and interior chamber dimensions of 2′ wide x 2′ high x 2′ long. The system has the capacity to heat 450 pounds of aluminum parts and the steel basket within 60

Quintus Technologies supplies high pressure Flexform press to airframe manufacturer

Quintus Technologies, Vasteras, Sweden, announced that they will supply a high pressure fluid cell press to France’s LAUAK Group, a Tier 1 supplier to the aerospace industry. The press will be installed at the LAUAK Aerostructures factory in Grandola, Portugal, in September 2023.  Reaffirming its continued commitment to productivity enhancement, LAUAK selected the Quintus model QFC 0.7×1.8-800 press with high pressure technology to bolster its manufacturing efficiency. “The forming press is undoubtedly at the heart

One Minute Mentor: Gas nitriding equipment

Gas nitriding and nitrocarburizing can be processed in horizontal or vertical chamber furnaces with refractory insulation. However, to allow a quick change of the atmosphere and to avoid influences resulting from previous processes in the same furnace, retort furnaces are preferred. To enable an acceptable production capacity, large vertical retort furnaces are used. The figure is a schematic sketch of a vertical retort furnace with a compensator for sealing against the atmosphere. Nowadays large horizontal