Skip to content

Lindberg/MPH ships mesh belt conveyor furnace for use with powdered metal

Lindberg/MPH, Mich., has announced the shipment of an electrically heated, full muffle, mesh belt conveyor furnace. This furnace is designed for treating pressed powdered material. The furnace is designed for applications with a maximum process temperature of 1000° C (1832° F) that utilize a nitrogen or clean dry filtered air process atmosphere. The unit is configured with 9 temperature control zones and includes a water-cooling section. The conveyor system features a 14 inch wide mesh

Seco/Warwick to supply a vacuum furnace specifically designed for the MRO industry

Seco/Warwick, Meadville, Pa., will supply a vacuum furnace specifically for the maintenance, repair, and operations (MRO) industry. The solution will be utilized for repair solutions for both complex aircraft engines and gas turbines for the energy industry in Hungary. The furnace on order is a unique solution due to the effective size of the heating chamber. It has been adapted to the AeroSpace Power requirements and has a working area of 1300 x 1000 x

Constellium joins EPA’s Energy Star program as an industrial partner

Constellium, Paris,  announced that they are participating in the U.S. Environmental Protection Agency (EPA) Energy Star program as an Industrial Partner. The Energy Star program is a voluntary initiative that helps businesses protect the environment by promoting energy-efficient products, homes, buildings and manufacturing plants, as well as save on energy costs. As an Industrial Partner, Constellium will work closely with the EPA to identify and implement energy-saving strategies and technologies across its manufacturing operations in

One Minute Mentor: Salt Bath Nitrocarburizing

Salt bath nitrocarburizing is usually performed at temperatures between 560 and 580 °C (1040 to 1075 °F) in cyanate- and carbonate-containing salts with traces of cyanides and furnaces similar to those used for the nitrocarburizing of mechanical compounds. These conditions fit well with the usual tempering temperatures of hot-work tool steels, which form the main field of application of salt bath nitrocarburizing in tooling with treatment times of 15 min to 2 h.  To guarantee

Can-Eng Furnaces contracted for continuous quench and temper furnace system

Can-Eng Furnaces International Ltd., Niagara, Ontario, was recently contracted to engineer and commission a continuous quench and temper furnace system for a North American producer of mining, construction, and materials handling products. The purchase of this equipment is part of a larger plant expansion and initiative to bring foreign outsourced manufacturing in house.   This move is not only to improve part quality but also to help eliminate overall shipping costs and reduce supply chain issues

Ipsen installs vacuum furnace at Taiwan Hodaka Technology

Ipsen, Tainan City, Taiwan, has announced the installation of a TurboTreater vacuum furnace for a customer in Southeast Asia. Established in 2002, Taiwan Hodaka Technology Co., Ltd. is an aluminum extrusion supplier, specializing in high-end aerospace aluminum alloys.  They also produce products used in the sporting goods, consumer electronics and automotive industries. The TurboTreater boasts a work zone size of 36” (914 mm) x 36” (914 mm) x 48” (1219mm) with a weight capacity of