Solar Atmospheres of Western PA treats a record load of titanium

Solar Atmospheres of Western PA, Hermitage, vacuum degassed a record 175,000 pounds of 6Al-4V titanium in their 48-foot-long vacuum furnace. The furnace load consisted of 154 sheets of titanium 40” wide X 240” long. It represented the largest and heaviest single load of titanium ever processed in Solar’s history. Bob Hill, president of Solar Atmospheres of Western PA states, “The future of the global aerospace titanium market is very promising with the many opportunities in

Kanthal and Rath announce strategic partnership to expand sustainable industrial heating technology offerings

Kanthal and Rath, Amherst, NY, have announced a strategic partnership aimed at expanding their combined offering in industrial heating technology. This collaboration is set to benefit industries such as steel and petrochemical as they strive to transition to greener practices. By joining forces, Kanthal and Rath will create the most extensive range of sustainable industrial heating solutions available in the market. Kanthal’s expertise in heating elements and systems, combined with Rath’s premium insulation and refractory

One Minute Mentor: Vacuum Furnaces

The demands on vacuum-hardening technology have changed in recent decades. One of the most important considerations that must be met is the accomplishment of highest dimensional stability with optimal microstructural properties and minimal change of the surface of the workpieces.  Minimizing exposure to air during the heat treatment by reducing the quantity of oxygen in a heat treatment furnace, as with creating a vacuum, is an excellent method for preventing changes in surface appearance and

EndoFlex generator chosen for fastener heat treatment

UPC-Marathon, Quebec,, a Nitrex company, has commissioned a 100 M3H EndoFlex endothermic gas generator for a South American manufacturer of industrial fasteners. This is a repeat customer that has UPC-Marathon‘s gas panels, flowmeters, oxygen probes, and Protherm plant automation software installed in their heat treatment operations. With the addition of the EndoFlex generator, they will now be able to supply gas to a new continuous mesh belt neutral hardening furnace for the treatment of metal

Constellium to provide closed-loop recycling for the all-new Megane E-TECH Electric

Constellium, Paris,  announced today its agreement with Renault Group to establish a closed-loop recycling process for the all-new Megane E-TECH Electric.  Aluminum, lightweight and fully recyclable, is the material of choice for the electrification of the automotive fleet, and Constellium is well-positioned to support this transition with advanced products and solutions. Renault Group has developed a closed-loop recycling process to bring manufacturing scrap from the stamping process directly back to Constellium, resulting in a reduced

Dr. Kathy Hayrynen awarded the 2023 Fred Linebarger teaching award

Dr. Kathy Hayrynen, FASM, vice president of research and development, Aalberts Surface Technologies, Cleveland, has been awarded the 2023 Fred Linebarger Teaching Award by the Cast Iron Division of the American Foundry Society Technical Council. The award was established in 2015 and honors the late Dr. Fred Linebarger (Director of Technology for Miller & CO) who devoted his career to the development of treatment alloys and processes for the production of both ductile and compacted