Skip to content

Seco/Vacuum ships Vector vacuum furnace for specialized nuclear operations

Seco/Vacuum, Pa., has shipped a single chamber high-pressure quench vacuum furnace, the Vector, to be utilized for a variety of heat-treating processes, including hardening of tool steels as well as high vacuum sintering and annealing.

Lindberg ships exothermic gas atmosphere generator to the manufacturing industry

Lindberg/MPH, MI, has announced the shipment of one gas-fired Exothermic atmosphere generator to the manufacturing industry.This exothermic generator features an energy efficient design that provides reliable and economic operation.

One Minute Mentor: Preheating for Austenitizing

Preheating normally is employed as a safeguard against the cracking and extreme distortion resulting from the thermal shock undergone by a cold workpiece when it is exposed to the high temperature of the austenitizing furnace.

Perryman Company expands titanium melting capacity by 60%

Perryman Company, Houston, Pa., will substantially increase its titanium melting capacity through additional electron beam and vacuum arc remelt furnaces. The furnaces will be located in Washington County, Pa.

Steel Dynamics announces new state-of-the-art low carbon aluminum flat rolled mill

Steel Dynamics, Fort Wayne, Ind, announced that it will construct and operate a 650,000-tonne low-carbon, recycled aluminum flat rolled mill, with two supporting satellite recycled aluminum slab centers. The capital investment is estimated to be $2.2 billion for the three facilities, and commercial production is planned to begin in the first quarter 2025.

Constellium achieves highest EcoVadis Platinum sustainability rating

Constellium, Paris, has received a Platinum rating from EcoVadis, a leading provider of business sustainability ratings, for a consecutive time. EcoVadis places the company in the top 1% of the 90,000 companies assessed worldwide.