Super Systems completes heat treating modernization of Milacron manufacturing facility

SuperSystems Inc., Cincinnati, recently completed major upgrades to the heat treating assets at Milacron LLC in Mt. Orab, Ohio, installing the latest furnaces and equipment, state-of-the-art controls, and modern SCADA infrastructure.

ASM member George Durfee to receive the ITA 2019 Lifetime Achievement Award

The International Titanium Association (ITA), Denver, Colo., announces that metallurgist George L. Durfee has been named the recipient of the ITA’s 2019 Lifetime Achievement Award.

Cleveland-Cliffs invests $100 million in DR iron plant, $830 million in HB iron plant

Cleveland-Cliffs Inc., Cleveland, announces that has started up its new production equipment, including supporting infrastructure, to support large-scale commercial production of DR-grade iron pellets at its Northshore Mining facility in Babbitt, Minnesota.

Aeromet aluminum A20X additive manufacturing alloy exceeds 500 MPa ultimate strength

Aeromet International Ltd., United Kingdom, announces that A20X, the aluminum alloy developed and patented by Aeromet, has cemented its status one of the strongest aluminum additive manufacturing powders commercially available after surpassing the key 500 MPa UTS mark.

One Minute Mentor: Cooling time and transformation diagram for a 52100 Jominy test bar

Figure 8 shows a cooling time and transformation (CTT) diagram for a 52100 Jominy test-bar sample austenitized at 845°C (1550°F).

Lindberg hot stamping furnace features one low-heat and three high-heat stacked chambers

Lindberg MPH, Riverside, Mich., has shipped an electrically heated four chamber hot-stamping furnace to the Gestamp Research and Development facility located in Auburn Hills, Mich.