{"id":12666,"date":"2023-04-05T00:20:05","date_gmt":"2023-04-05T00:20:05","guid":{"rendered":"https:\/\/staging.asminternational.org\/hts-new\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/"},"modified":"2023-06-08T20:02:52","modified_gmt":"2023-06-08T20:02:52","slug":"one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips","status":"publish","type":"post","link":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/","title":{"rendered":"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips"},"content":{"rendered":"<p><span style=\"font-weight: 400\">The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed. Strip dimensions range between 10 to 750 mm (0.4 to 29.5 in.) wide and 0.05 to 4 mm (0.002 to 0.16 in.) thick. High quenching rates are necessary, especially for plain carbon steels. Cooling gradients of up to 600 K\/s are possible in a molten lead-bismuth quench. Because two-stage quenching technology provides considerable advantages over quenching in oil, this method has been adopted worldwide. It is also possible to achieve isothermal transformation to bainite and pearlite using a molten metal quench, so this type of hardening and tempering line is extremely versatile.<\/span><\/p>\n<p><span style=\"font-weight: 400\">The configuration of a high-performance line involves an entry and exit section of the strip handling equipment (Fig. 10). The hardening section consists of the austenitizing furnace, the molten metal quench or hydrogen quench, and a martensite cooler. Beyond the martensite cooler the strip is martensitic and fully hardened, and then it passes through the tempering section\u2014consisting of a leveling furnace, tempering furnace equipped with an atmosphere recirculation system, and an atmosphere jet cooler\u2014to finally leave the facility, completely flat, with a bright surface finish and tempered to very uniform tensile strength.<\/span><\/p>\n<p><span style=\"font-weight: 400\">For more information, click on the link below (subscription required). Then scroll to Figure 10<\/span><\/p>\n<p><span>R Schneider ; R. Mesquita ; H. Altena ; T. M\u00fcller ; P. Seemann,Processes and Furnace Equipment for Heat Treating of Tool Steels, ASM International, 2014, <\/span><a href=\"https:\/\/doi.org\/10.31399\/asm.hb.v04d.a0005958\"><span>https:\/\/doi.org\/10.31399\/asm.hb.v04d.a0005958<\/span><\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed. Strip dimensions range [&hellip;]<\/p>\n","protected":false},"author":59508,"featured_media":12667,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"categories":[489,502,465,475,476,441],"tags":[],"class_list":["post-12666","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-annealing","category-cast-irons","category-coating-microstructures-and-properties","category-furnace-atmospheres","category-furnaces-and-equipment","category-news-articles"],"yoast_head":"<!-- This site is optimized with the Yoast SEO plugin v27.9 - https:\/\/yoast.com\/product\/yoast-seo-wordpress\/ -->\n<title>One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips - Heat Treating Society<\/title>\n<meta name=\"description\" content=\"The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/\" \/>\n<meta property=\"og:locale\" content=\"en_US\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips - Heat Treating Society\" \/>\n<meta property=\"og:description\" content=\"The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/\" \/>\n<meta property=\"og:site_name\" content=\"Heat Treating Society\" \/>\n<meta property=\"article:published_time\" content=\"2023-04-05T00:20:05+00:00\" \/>\n<meta property=\"article:modified_time\" content=\"2023-06-08T20:02:52+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/staging.asminternational.org\/app\/uploads\/sites\/85\/2023\/04\/HtPro_enews_041123_OMM_250.png\" \/>\n\t<meta property=\"og:image:width\" content=\"250\" \/>\n\t<meta property=\"og:image:height\" content=\"96\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/png\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Written by\" \/>\n\t<meta name=\"twitter:data1\" content=\"\" \/>\n\t<meta name=\"twitter:label2\" content=\"Est. reading time\" \/>\n\t<meta name=\"twitter:data2\" content=\"1 minute\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"Article\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/\"},\"author\":{\"name\":\"\",\"@id\":\"\"},\"headline\":\"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips\",\"datePublished\":\"2023-04-05T00:20:05+00:00\",\"dateModified\":\"2023-06-08T20:02:52+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/\"},\"wordCount\":282,\"publisher\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#organization\"},\"image\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/#primaryimage\"},\"thumbnailUrl\":\"https:\\\/\\\/cdn-prd-main.asm-media.cloud\\\/uploads\\\/sites\\\/85\\\/2023\\\/04\\\/HtPro_enews_041123_OMM_250.png\",\"articleSection\":[\"Annealing\",\"Cast Irons\",\"Coating Microstructures and Properties\",\"Furnace Atmospheres\",\"Furnaces and Equipment\",\"News Articles\"],\"inLanguage\":\"en-US\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/\",\"url\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/\",\"name\":\"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips - Heat Treating Society\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/#primaryimage\"},\"image\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/#primaryimage\"},\"thumbnailUrl\":\"https:\\\/\\\/cdn-prd-main.asm-media.cloud\\\/uploads\\\/sites\\\/85\\\/2023\\\/04\\\/HtPro_enews_041123_OMM_250.png\",\"datePublished\":\"2023-04-05T00:20:05+00:00\",\"dateModified\":\"2023-06-08T20:02:52+00:00\",\"description\":\"The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/#breadcrumb\"},\"inLanguage\":\"en-US\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"en-US\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/#primaryimage\",\"url\":\"https:\\\/\\\/cdn-prd-main.asm-media.cloud\\\/uploads\\\/sites\\\/85\\\/2023\\\/04\\\/HtPro_enews_041123_OMM_250.png\",\"contentUrl\":\"https:\\\/\\\/cdn-prd-main.asm-media.cloud\\\/uploads\\\/sites\\\/85\\\/2023\\\/04\\\/HtPro_enews_041123_OMM_250.png\",\"width\":250,\"height\":96},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"Home\",\"item\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#website\",\"url\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/\",\"name\":\"Heat Treating Society\",\"description\":\"Heat Treating Society ASM International\",\"publisher\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"en-US\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#organization\",\"name\":\"Heat Treating Society\",\"url\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"en-US\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/cdn-prd-main.asm-media.cloud\\\/uploads\\\/sites\\\/85\\\/2022\\\/06\\\/layout_set_logo.png\",\"contentUrl\":\"https:\\\/\\\/cdn-prd-main.asm-media.cloud\\\/uploads\\\/sites\\\/85\\\/2022\\\/06\\\/layout_set_logo.png\",\"width\":286,\"height\":95,\"caption\":\"Heat Treating Society\"},\"image\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#\\\/schema\\\/logo\\\/image\\\/\"}},{\"@type\":\"Person\",\"@id\":\"\",\"url\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/author\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO plugin. -->","yoast_head_json":{"title":"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips - Heat Treating Society","description":"The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/","og_locale":"en_US","og_type":"article","og_title":"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips - Heat Treating Society","og_description":"The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed.","og_url":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/","og_site_name":"Heat Treating Society","article_published_time":"2023-04-05T00:20:05+00:00","article_modified_time":"2023-06-08T20:02:52+00:00","og_image":[{"width":250,"height":96,"url":"https:\/\/staging.asminternational.org\/app\/uploads\/sites\/85\/2023\/04\/HtPro_enews_041123_OMM_250.png","type":"image\/png"}],"twitter_card":"summary_large_image","twitter_misc":{"Written by":"","Est. reading time":"1 minute"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"Article","@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/#article","isPartOf":{"@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/"},"author":{"name":"","@id":""},"headline":"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips","datePublished":"2023-04-05T00:20:05+00:00","dateModified":"2023-06-08T20:02:52+00:00","mainEntityOfPage":{"@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/"},"wordCount":282,"publisher":{"@id":"https:\/\/staging.asminternational.org\/hts\/#organization"},"image":{"@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/#primaryimage"},"thumbnailUrl":"https:\/\/cdn-prd-main.asm-media.cloud\/uploads\/sites\/85\/2023\/04\/HtPro_enews_041123_OMM_250.png","articleSection":["Annealing","Cast Irons","Coating Microstructures and Properties","Furnace Atmospheres","Furnaces and Equipment","News Articles"],"inLanguage":"en-US"},{"@type":"WebPage","@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/","url":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/","name":"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips - Heat Treating Society","isPartOf":{"@id":"https:\/\/staging.asminternational.org\/hts\/#website"},"primaryImageOfPage":{"@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/#primaryimage"},"image":{"@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/#primaryimage"},"thumbnailUrl":"https:\/\/cdn-prd-main.asm-media.cloud\/uploads\/sites\/85\/2023\/04\/HtPro_enews_041123_OMM_250.png","datePublished":"2023-04-05T00:20:05+00:00","dateModified":"2023-06-08T20:02:52+00:00","description":"The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed.","breadcrumb":{"@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/#breadcrumb"},"inLanguage":"en-US","potentialAction":[{"@type":"ReadAction","target":["https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/"]}]},{"@type":"ImageObject","inLanguage":"en-US","@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/#primaryimage","url":"https:\/\/cdn-prd-main.asm-media.cloud\/uploads\/sites\/85\/2023\/04\/HtPro_enews_041123_OMM_250.png","contentUrl":"https:\/\/cdn-prd-main.asm-media.cloud\/uploads\/sites\/85\/2023\/04\/HtPro_enews_041123_OMM_250.png","width":250,"height":96},{"@type":"BreadcrumbList","@id":"https:\/\/staging.asminternational.org\/hts\/one-minute-mentor-continuous-operating-furnaces-for-tool-steel-strips\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https:\/\/staging.asminternational.org\/hts\/"},{"@type":"ListItem","position":2,"name":"One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips"}]},{"@type":"WebSite","@id":"https:\/\/staging.asminternational.org\/hts\/#website","url":"https:\/\/staging.asminternational.org\/hts\/","name":"Heat Treating Society","description":"Heat Treating Society ASM International","publisher":{"@id":"https:\/\/staging.asminternational.org\/hts\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/staging.asminternational.org\/hts\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"en-US"},{"@type":"Organization","@id":"https:\/\/staging.asminternational.org\/hts\/#organization","name":"Heat Treating Society","url":"https:\/\/staging.asminternational.org\/hts\/","logo":{"@type":"ImageObject","inLanguage":"en-US","@id":"https:\/\/staging.asminternational.org\/hts\/#\/schema\/logo\/image\/","url":"https:\/\/cdn-prd-main.asm-media.cloud\/uploads\/sites\/85\/2022\/06\/layout_set_logo.png","contentUrl":"https:\/\/cdn-prd-main.asm-media.cloud\/uploads\/sites\/85\/2022\/06\/layout_set_logo.png","width":286,"height":95,"caption":"Heat Treating Society"},"image":{"@id":"https:\/\/staging.asminternational.org\/hts\/#\/schema\/logo\/image\/"}},{"@type":"Person","@id":"","url":"https:\/\/staging.asminternational.org\/hts\/author\/"}]}},"acf":[],"_links":{"self":[{"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/posts\/12666","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/users\/59508"}],"replies":[{"embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/comments?post=12666"}],"version-history":[{"count":0,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/posts\/12666\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/media\/12667"}],"wp:attachment":[{"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/media?parent=12666"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/categories?post=12666"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/tags?post=12666"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}