{"id":9173,"date":"2014-12-10T04:20:55","date_gmt":"2014-12-10T04:20:55","guid":{"rendered":"https:\/\/staging.asminternational.org\/hts-new\/results\/-\/journal_content\/56\/10192\/23330613\/NEWS\/"},"modified":"2023-02-07T04:49:48","modified_gmt":"2023-02-07T04:49:48","slug":"ultrasound-treatment-removes-hydrogen-from-molten-aluminum","status":"publish","type":"post","link":"https:\/\/staging.asminternational.org\/hts\/ultrasound-treatment-removes-hydrogen-from-molten-aluminum\/","title":{"rendered":"Ultrasound treatment removes hydrogen from molten aluminum"},"content":{"rendered":"<p>\n\tResearchers at Brunel University London report that an ultrasound treatment could be a much cheaper and more environmentally friendly way to remove hydrogen from aluminum alloys than conventional methods. &nbsp;Treating molten metal with ultrasound is a cleaner, greener and more efficient route to produce high quality castings<\/p>\n<p>\n\tMolten aluminum alloys at 700\u00b0C naturally contain a high percentage of dissolved hydrogen. Left untreated, the resulting solid metal is highly porous. The most widely- used method of hydrogen removal \u2013 argon rotary degassing &#8211; is energy intensive and requires costly components.<\/p>\n<p>\n\tIn pilot scale trials funded by EU Framework Seven Programme, the team found that ultrasound was just as efficient as the standard method, but produced far less waste material (dross). The price of argon gas continues to rise because making it requires producers to liquefy air, which takes a lot of energy.<\/p>\n<p>\n\tResearch with quantities of up to 150 kg confirmed earlier laboratory tests that a moving ultrasound probe could achieve results similar to those of the argon process, but with the advantages of not relying on expensive and fragile graphite rods and expensive gas which cannot be captured and recycled. The five-fold reduction of the amount of dross created is another benefit.<\/p>\n<p>\n\t<a href=\"http:\/\/www.brunel.ac.uk\/\">http:\/\/www.brunel.ac.uk\/<\/a><\/p>\n<p>\n\t&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>Researchers at Brunel University London report that an ultrasound treatment could be a much cheaper and more environmentally friendly way to remove hydrogen from aluminum alloys than conventional methods.<\/p>\n","protected":false},"author":63082,"featured_media":0,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"categories":[439,440,441,1],"tags":[],"class_list":["post-9173","post","type-post","status-publish","format-standard","hentry","category-general","category-news","category-news-articles","category-uncategorized"],"yoast_head":"<!-- This site is optimized with the Yoast SEO plugin v27.9 - https:\/\/yoast.com\/product\/yoast-seo-wordpress\/ -->\n<title>Ultrasound treatment removes hydrogen from molten aluminum - Heat Treating Society<\/title>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/\" \/>\n<meta property=\"og:locale\" content=\"en_US\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Ultrasound treatment removes hydrogen from molten aluminum - Heat Treating Society\" \/>\n<meta property=\"og:description\" content=\"Researchers at Brunel University London report that an ultrasound treatment could be a much cheaper and more environmentally friendly way to remove hydrogen from aluminum alloys than conventional methods.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/\" \/>\n<meta property=\"og:site_name\" content=\"Heat Treating Society\" \/>\n<meta property=\"article:published_time\" content=\"2014-12-10T04:20:55+00:00\" \/>\n<meta property=\"article:modified_time\" content=\"2023-02-07T04:49:48+00:00\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Written by\" \/>\n\t<meta name=\"twitter:data1\" content=\"\" \/>\n\t<meta name=\"twitter:label2\" content=\"Est. reading time\" \/>\n\t<meta name=\"twitter:data2\" content=\"1 minute\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"Article\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/results\\\/-\\\/journal_content\\\/56\\\/10192\\\/23330548\\\/NEWS\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/results\\\/-\\\/journal_content\\\/56\\\/10192\\\/23330548\\\/NEWS\\\/\"},\"author\":{\"name\":\"\",\"@id\":\"\"},\"headline\":\"Ultrasound treatment removes hydrogen from molten aluminum\",\"datePublished\":\"2014-12-10T04:20:55+00:00\",\"dateModified\":\"2023-02-07T04:49:48+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/results\\\/-\\\/journal_content\\\/56\\\/10192\\\/23330548\\\/NEWS\\\/\"},\"wordCount\":214,\"publisher\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#organization\"},\"articleSection\":[\"general\",\"news\",\"News Articles\"],\"inLanguage\":\"en-US\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/results\\\/-\\\/journal_content\\\/56\\\/10192\\\/23330548\\\/NEWS\\\/\",\"url\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/results\\\/-\\\/journal_content\\\/56\\\/10192\\\/23330548\\\/NEWS\\\/\",\"name\":\"Ultrasound treatment removes hydrogen from molten aluminum - Heat Treating Society\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#website\"},\"datePublished\":\"2014-12-10T04:20:55+00:00\",\"dateModified\":\"2023-02-07T04:49:48+00:00\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/results\\\/-\\\/journal_content\\\/56\\\/10192\\\/23330548\\\/NEWS\\\/#breadcrumb\"},\"inLanguage\":\"en-US\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/results\\\/-\\\/journal_content\\\/56\\\/10192\\\/23330548\\\/NEWS\\\/\"]}]},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/results\\\/-\\\/journal_content\\\/56\\\/10192\\\/23330548\\\/NEWS\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"Home\",\"item\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Ultrasound treatment removes hydrogen from molten aluminum\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#website\",\"url\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/\",\"name\":\"Heat Treating Society\",\"description\":\"Heat Treating Society ASM International\",\"publisher\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"en-US\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#organization\",\"name\":\"Heat Treating Society\",\"url\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"en-US\",\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/cdn-prd-main.asm-media.cloud\\\/uploads\\\/sites\\\/85\\\/2022\\\/06\\\/layout_set_logo.png\",\"contentUrl\":\"https:\\\/\\\/cdn-prd-main.asm-media.cloud\\\/uploads\\\/sites\\\/85\\\/2022\\\/06\\\/layout_set_logo.png\",\"width\":286,\"height\":95,\"caption\":\"Heat Treating Society\"},\"image\":{\"@id\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/#\\\/schema\\\/logo\\\/image\\\/\"}},{\"@type\":\"Person\",\"@id\":\"\",\"url\":\"https:\\\/\\\/staging.asminternational.org\\\/hts\\\/author\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO plugin. -->","yoast_head_json":{"title":"Ultrasound treatment removes hydrogen from molten aluminum - Heat Treating Society","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/","og_locale":"en_US","og_type":"article","og_title":"Ultrasound treatment removes hydrogen from molten aluminum - Heat Treating Society","og_description":"Researchers at Brunel University London report that an ultrasound treatment could be a much cheaper and more environmentally friendly way to remove hydrogen from aluminum alloys than conventional methods.","og_url":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/","og_site_name":"Heat Treating Society","article_published_time":"2014-12-10T04:20:55+00:00","article_modified_time":"2023-02-07T04:49:48+00:00","twitter_card":"summary_large_image","twitter_misc":{"Written by":"","Est. reading time":"1 minute"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"Article","@id":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/#article","isPartOf":{"@id":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/"},"author":{"name":"","@id":""},"headline":"Ultrasound treatment removes hydrogen from molten aluminum","datePublished":"2014-12-10T04:20:55+00:00","dateModified":"2023-02-07T04:49:48+00:00","mainEntityOfPage":{"@id":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/"},"wordCount":214,"publisher":{"@id":"https:\/\/staging.asminternational.org\/hts\/#organization"},"articleSection":["general","news","News Articles"],"inLanguage":"en-US"},{"@type":"WebPage","@id":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/","url":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/","name":"Ultrasound treatment removes hydrogen from molten aluminum - Heat Treating Society","isPartOf":{"@id":"https:\/\/staging.asminternational.org\/hts\/#website"},"datePublished":"2014-12-10T04:20:55+00:00","dateModified":"2023-02-07T04:49:48+00:00","breadcrumb":{"@id":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/#breadcrumb"},"inLanguage":"en-US","potentialAction":[{"@type":"ReadAction","target":["https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/"]}]},{"@type":"BreadcrumbList","@id":"https:\/\/staging.asminternational.org\/hts\/results\/-\/journal_content\/56\/10192\/23330548\/NEWS\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https:\/\/staging.asminternational.org\/hts\/"},{"@type":"ListItem","position":2,"name":"Ultrasound treatment removes hydrogen from molten aluminum"}]},{"@type":"WebSite","@id":"https:\/\/staging.asminternational.org\/hts\/#website","url":"https:\/\/staging.asminternational.org\/hts\/","name":"Heat Treating Society","description":"Heat Treating Society ASM International","publisher":{"@id":"https:\/\/staging.asminternational.org\/hts\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/staging.asminternational.org\/hts\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"en-US"},{"@type":"Organization","@id":"https:\/\/staging.asminternational.org\/hts\/#organization","name":"Heat Treating Society","url":"https:\/\/staging.asminternational.org\/hts\/","logo":{"@type":"ImageObject","inLanguage":"en-US","@id":"https:\/\/staging.asminternational.org\/hts\/#\/schema\/logo\/image\/","url":"https:\/\/cdn-prd-main.asm-media.cloud\/uploads\/sites\/85\/2022\/06\/layout_set_logo.png","contentUrl":"https:\/\/cdn-prd-main.asm-media.cloud\/uploads\/sites\/85\/2022\/06\/layout_set_logo.png","width":286,"height":95,"caption":"Heat Treating Society"},"image":{"@id":"https:\/\/staging.asminternational.org\/hts\/#\/schema\/logo\/image\/"}},{"@type":"Person","@id":"","url":"https:\/\/staging.asminternational.org\/hts\/author\/"}]}},"acf":[],"_links":{"self":[{"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/posts\/9173","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/users\/63082"}],"replies":[{"embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/comments?post=9173"}],"version-history":[{"count":0,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/posts\/9173\/revisions"}],"wp:attachment":[{"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/media?parent=9173"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/categories?post=9173"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/staging.asminternational.org\/hts\/wp-json\/wp\/v2\/tags?post=9173"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}