LECO, St. Joseph, Mich., is working to develop a new test method for carbon, low-alloy, and free-machining steel by glow discharge atomic emission spectrometry through ASTM International.
ASTM International, formerly known as the American Society for Testing and Materials, is globally recognized as one of the most respected standards development organizations. Standards are developed through the consensus process, with around 150 committees (and over 2100 subcommittees) participating. Over 150 major global industries are driven by standards crafted through ASTM, including metallography, coal and coke, additive manufacturing technologies, plastics, and more. According to astm.org, 12,000 ASTM standards are used today around the world to improve product quality, enhance health and safety, strengthen market access and trade, and build consumer confidence.
LECO participates in six ASTM committees as part of our commitment to empower results and help labs worldwide.
• Committee E01: Analytical Chemistry for Metals, Ores, and Related Materials
• Committee D05: Coal and Coke
• Committee F42: Additive Manufacturing Technologies
• Committee C26: Nuclear Fuel Cycle
• Committee C07: Lime and Limestone
• Committee D02: Petroleum Products, Liquid Fuels, and Lubricants
The company’s main goal in participating is to have an active voice and be involved in the development of standards and guides that relate to the analyzers and other instrumentation that we produce. As part of these committees, LECO can provide technical expertise on equipment and their relative applications to various materials.
LECO’s work is currently focused on developing a new test method for analysis of carbon, low-alloy, and free-machining steel by glow discharge atomic emission spectrometry (GD-AES). For this method, specimens to be analyzed may be in the form of a disk, casting, foil, sheet, plate, extrusion, or some other wrought form or shape. There is currently no standard test method for this type of analysis, but there is a need. To see LECO’s current low-alloy method, fill out the form here.
LECO will also soon be inviting collaborators to the Inter-Laboratory Study for this draft method. If you currently use GD-AES equipment, LECO welcomes you to be involved. If interested, send a message to [email protected] and make a reference to this post.