A team of scientists at the Department of Energy’s Oak Ridge National Laboratory has developed a new method to process nanocellulose, a plant-based material, reducing energy needs by 21%. This method, discovered through molecular simulations and pilot testing, uses a solvent of sodium hydroxide and urea in water, significantly lowering production costs of nanocellulosic fiber, a strong, lightweight biomaterial ideal for 3D-printing sustainable structures. The findings, achieved in collaboration with the University of Tennessee and the University of Maine, support a circular bioeconomy by replacing petroleum-based resources with renewable, biodegradable materials, thus decarbonizing the economy and reducing waste.
The scientists pursued more efficient fibrillation, the process of separating cellulose into nanofibrils, traditionally an energy-intensive, high-pressure mechanical procedure occurring in an aqueous pulp suspension. The researchers tested eight candidate solvents to determine which would function as a better pretreatment for cellulose. They used computer models that mimic the behavior of atoms and molecules in the solvents and cellulose as they move and interact. The approach simulated about 0.6 million atoms, giving scientists an understanding of the complex process without the need for initial, time-consuming physical work in the lab.
The simulations developed by researchers with the UT-ORNL Center for Molecular Biophysics, or CMB, and the Chemical Sciences Division at ORNL were run on the Frontier exascale computing system — the world’s fastest supercomputer for open science. Frontier is part of the Oak Ridge Leadership Computing Facility, a DOE Office of Science user facility at ORNL.
“These simulations, looking at every single atom and the forces between them, provide detailed insight into not just whether a process works, but exactly why it works,” said project lead Jeremy Smith, director of the CMB and a UT-ORNL Governor’s Chair.
Once the best candidate was identified, the scientists followed up with pilot-scale experiments that confirmed the solvent pretreatment resulted in an energy savings of 21% compared to using water alone.
With the winning solvent, researchers estimated an electricity savings potential of about 777-kilowatt hours per metric ton of cellulose nanofibrils, or CNF, which is roughly the equivalent of the amount needed to power a house for a month. Testing of the resulting fibers at the Center for Nanophase Materials Science, a DOE Office of Science user facility at ORNL, and U-Maine found similar mechanical strength and other desirable characteristics compared with conventionally produced CNF.
“We targeted the separation and drying process since it is the most energy-intense stage in creating nanocellulosic fiber,” said Monojoy Goswami of ORNL’s Carbon and Composites group. “Using these molecular dynamics simulations and our high-performance computing at Frontier, we were able to accomplish quickly what might have taken us years in trial-and-error experiments.”
“When we combine our computational, materials science and manufacturing expertise and nanoscience tools at ORNL with the knowledge of forestry products at the University of Maine, we can take some of the guessing game out of science and develop more targeted solutions for experimentation,” said Soydan Ozcan, lead for the Sustainable Manufacturing Technologies group at ORNL.
The project is supported by both the DOE Office of Energy Efficiency and Renewable Energy’s Advanced Materials and Manufacturing Technologies Office, or AMMTO, and by the partnership of ORNL and U-Maine known as the Hub & Spoke Sustainable Materials & Manufacturing Alliance for Renewable Technologies Program, or SM2ART.
The SM2ART program focuses on developing an infrastructure-scale factory of the future, where sustainable, carbon-storing biomaterials are used to build everything from houses, ships and automobiles to clean energy infrastructure such as wind turbine components, Ozcan said.
“Creating strong, affordable, carbon-neutral materials for 3D printers gives us an edge to solve issues like the housing shortage,” Smith said.
It typically takes about six months to build a house using conventional methods. But with the right mix of materials and additive manufacturing, producing and assembling sustainable, modular housing components could take just a day or two, the scientists added.
The team continues to pursue additional pathways for more cost-effective nanocellulose production, including new drying processes. Follow-on research is expected to use simulations to also predict the best combination of nanocellulose and other polymers to create fiber-reinforced composites for advanced manufacturing systems such as the ones being developed and refined at DOE’s Manufacturing Demonstration Facility, or MDF, at ORNL. The MDF, supported by AMMTO, is a nationwide consortium of collaborators working with ORNL to innovate, inspire and catalyze the transformation of U.S. manufacturing.
For more information: PNAS
Image: ORNL scientists used molecular dynamics simulations, exascale computing, lab testing and analysis to accelerate the development of an energy-saving method to produce nanocellulosic fibers. This strong, lightweight, material is ideal for 3D-printing of sustainable housing, vehicles and clean energy components.