Creating the batteries or electronics of the future requires understanding materials that are just a few atoms thick and that change their fundamental physical properties in fractions of a second. Cutting-edge facilities at the Department of Energy’s SLAC National Accelerator Laboratory and Stanford University, both in Calif., allow researchers to visualize properties of these nanoscale materials at ultrafast time scales.
In one experiment, a team led by Aaron Lindenberg shows atoms shifting in trillionths of a second to produce a wrinkle in a three-atom-thick sample of a material that might someday be used in flexible electronics. Another study observed semiconductor crystals—called quantum dots because they defy classical physics at the nanoscale—expand and shrink in response to ultrafast pulses of laser light.
Revealing such intriguing properties at the nanoscale gives clues about the fundamental nature of materials and how they perform in applications we rely on for energy or information.
“Even though some of these materials are completely embedded in everyday technologies, not a lot is understood about how they work,” says Lindenberg, who is an associate professor of materials science and engineering. “Part of the reason some phenomena are not well understood is because they happen so fast—in billionths, trillionths or even quadrillionths of a second. For the first time, we have tools that allow us to see these things,” he says.
Working at the intersection of materials science and engineering, the team is focused on finding promising materials for next-generation electronics, light-based data storage technologies, and energy applications.
“There are a broad range of new properties that emerge at the nanoscale,” Lindenberg says. “The tiniest samples, with just tens or hundreds of atoms, can have nearly flawless structures that make them ideal test tubes for very fundamental questions about what happens when a material transforms.”
The team uses different types of laser light to learn how simple tweaks in the size, shape, and design of materials can change their basic properties in unexpected ways, which could lead to new applications. Taking advantage of the powerful x-rays at SLAC facilities, they explore ultrafast changes in nanoscale samples.
“We are trying to understand how electrons or atoms move in materials, which in turn determines, for example, the efficiency of solar cells and other energy-related materials, and how materials switch between different forms,” he says. “Ultrafast techniques allow you to see these kinds of things in a completely new way.”
Image caption — A new techniques developed at SLAC and Stanford allow scientists to observe changes at the nanoscale that occur in fractions of a second in response to light. This artist’s conception depicts the first step in the photovoltaic response that light produces in lead titanate.