Researchers from North Carolina State University, Raleigh, and Qatar University developed a new high-entropy metal alloy that has a higher strength-to-weight ratio than any other existing metal material.
High-entropy alloys are materials that consist of five or more metals in approximately equal amounts. They the focus of significant attention in materials science and engineering because they can have desirable properties. The research team combined lithium, magnesium, titanium, aluminum, and scandium to make a nanocrystalline high-entropy alloy that has low density, but very high strength.
“The density is comparable to aluminum, but it is stronger than titanium alloys,” says Carl Koch, Kobe Steel Distinguished Professor of Materials Science and Engineering at NC State. “It has a combination of high strength and low density that is, as far as we can tell, unmatched by any other metallic material. The strength-to-weight ratio is comparable to some ceramics, but we think it’s tougher—less brittle—than ceramics.”
There are a wide range of uses for strong, lightweight materials, such as in vehicles or prosthetic devices. “We still have a lot of research to do to fully characterize this material and explore the best processing methods for it,” Koch says. At this point, the primary problem with the alloy is that it is made of 20% scandium, which is extremely expensive. “One thing we’ll be looking at is whether scandium can be replaced or eliminated from the alloy,” Koch says.
The work was supported in part by the National Science Foundation under grant number DMR-1104930.