Computations show that a material made with just the right amounts of hafnium, nitrogen, and carbon would have a melting point of more than 4400 K (7460°F). That’s about two-thirds the temperature at the surface of the sun and 200 K higher than the highest melting point ever recorded experimentally.
The experimental record-holder is a substance made from the elements hafnium, tantalum, and carbon (Hf-Ta-C). But these new calculations suggest that an optimal composition of hafnium, nitrogen, and carbon—HfN0.38C0.51—is a promising candidate to set a new mark. The next step, which the researchers are undertaking now, is to synthesize material and corroborate the findings in the lab.
“The advantage of starting with the computational approach is we can try lots of different combinations very inexpensively and find ones that might be worth experimenting with in the lab,” says Axel van de Walle, associate professor of engineering at Brown University. “Otherwise we’d just be shooting in the dark. Now we know we have something that’s worth a try.”
Researchers used a computational technique that infers melting points by simulating physical processes at the atomic level, following the law of quantum mechanics. The technique looks at the dynamics of melting as they occur at the nanoscale, in blocks of 100 or so atoms. It’s more efficient than traditional methods, but still computationally demanding due to the large number of potential compounds to test. The work was done using the National Science Foundation’s XSEDE computer network and Brown’s “Oscar” high-performance computer cluster.
The team analyzed the Hf-Ta-C material for which the melting point had already been experimentally determined. The simulation was able to elucidate some of the factors that contribute to the material’s remarkable heat tolerance.
The work shows that Hf-Ta-C combined a high heat of fusion (the energy released or absorbed when it transitions from solid to liquid) with a small difference between the entropies (disorder) of the solid and liquid phases. “What makes something melt is the entropy gained in the process of phase transformation,” van de Walle explains. “So if the entropy of the solid is already very high, that tends to stabilize the solid and increase the melting point.”
Researchers then used those findings to look for compounds that might maximize those properties. They found that a compound with hafnium, nitrogen, and carbon would have a similarly high heat of fusion but a smaller difference between the entropies of the solid and the liquid. When they calculated the melting point using their computational approach, it came out 200 K higher than the experimental record.
The group is now collaborating with Alexandra Navrotsky’s lab at the University of California, Davis, to synthesize the compound and perform the melting point experiments. Navrotksy’s lab is equipped for such high-temperature experiments.
Potential uses?
The work could ultimately point toward new high-performance materials for a variety of uses, from plating for gas turbines to heat shields on high-speed aircraft. But whether the HfN0.38C0.51 compound itself will be a useful material isn’t clear, van de Walle says.
“Melting point isn’t the only property that’s important [in material applications],” he says. “You would need to consider things like mechanical properties and oxidation resistance and all sorts of other properties. So taking those things into account you may want to mix other things with this that might lower the melting point. But since you’re already starting so high, you have more leeway to adjust other properties. So I think this gives people an idea of what can be done.”
The work also demonstrates the power of this relatively new computational technique, van de Walle says. In recent years, interest in using computation to explore the material properties of a large number of candidate compounds has increased, but much of that work has focused on properties that are far easier to compute than the melting point. “Melting point is a really difficult prediction problem compared to what has been done before,” van de Walle says. “For the modeling community, I think that’s what is special about this.”
Funding came from the U.S. Office of Naval Research and Brown University through the use of the facilities at its Center for Computation and Visualization. The Extreme Science and Engineering Discovery Environment (XSEDE), which was used in this study, is supported by National Science Foundation.