Nitrex, Quebec, announced that an automotive company in South America has placed a follow-up order for a second EndoFlex generator from UPC-Marathon, a Nitrex company. Following the successful installation of a 200 m³/h EndoFlex unit last year, the new generator, with a similar capacity, aims to enhance stability, ensure consistent composition and gas flows, and prioritize top-tier quality in automotive gear boxes while achieving efficiencies in heat treatment operations.
Before adopting the EndoFlex solution, the manufacturer relied on four outdated generator units, each with a capacity of 70 m³/h and consuming 80 kW of power. Remarkably, with the same 80 kW of power consumption, the EndoFlex generator delivers an impressive 200 m³/h capacity. This transition represents not only a remarkable 75% reduction in power consumption but also a significant boost in efficiency and cost-effectiveness for the customer.
The shift to EndoFlex also signifies a substantial contribution to operational efficiency and sustainability efforts. The new generator streamlines maintenance procedures, adheres to stringent quality standards, and reduces CO2 emissions. EndoFlex’s precision control over gas quality and production for the neutral hardening furnace enhances product quality, reduces operating costs, and optimizes energy consumption. By automatically adjusting gas production to match real-time furnace demand, EndoFlex effectively eliminates overproduction and waste.
This order underscores the automotive company’s commitment to leveraging advanced technologies for enhanced productivity and sustainability in their operations.