A new type of polymer membrane could replace expensive platinum in alkaline batteries and fuel cells. “We have tried to break this paradigm of tradeoffs in materials (by improving) both the stability and the conductivity of this membrane at the same time, and that is what we were able to do with this unique polymeric materials design,” says Michael Hickner, associate professor of materials science and engineering at Penn State University, University Park.
In solid-state alkaline fuel cells, anion exchange membranes conduct negative charges between the device’s cathode and anode-the negative and positive connections of the cell-to create useable electric power. Most fuel cells currently use membranes that require platinum-based catalysts that are effective but expensive.
Hickner’s new polymer is a unique anion exchange membrane-a new type of fuel cell and battery membrane-that allows the use of much more cost-efficient non-precious metal catalysts and does not compromise either durability or efficiency like previous anion exchange membranes. “What we’re really doing here is providing alternatives, possible choices, new technology so that people who want to commercialize fuel cells can now choose between the old paradigm and new possibilities with anion exchange membranes,” Hickner says.
Creating this alternative took some intuition and good fortune. In work spearheaded by Nanwen Li, a postdoctoral researcher in materials science and engineering, Hickner’s team created several variations of the membrane, each with slightly different chemical compositions. They then ran each variation under simulated conditions to predict which would be optimal in an actual fuel cell. The researchers report their findings in a recent issue of the Journal of the American Chemical Society.
Durable and efficient
Based on these initial tests, the group predicted that the membranes with long 16-carbon structures in their chemical makeup would provide the best efficiency and durability, as measured respectively by conductivity and long-term stability. The team then tested each possibility in an operating fuel cell device and measured the fuel cell’s output and lifetime for each material variation. Despite predictions, the membranes containing shorter six-carbon structures proved to be much more durable and efficient after 60 hours of continuous operation.
“We were somewhat surprised…that what we thought was the best material in our lab testing wasn’t necessarily the best material in the cell when it was evaluated over time,” says Hickner, who adds that researchers are still trying to understand why the 6-carbon variation has better long-term durability than the 16-carbon sample in the fuel cell by studying the operating conditions of the cell in detail.
Because the successful membrane was so much more effective than the initial lab studies predicted, researchers are now interested in accounting for the interactions that the membranes experienced while inside the cell.
“We have the fuel cell output-so we have the fuel cell efficiency, the fuel cell life time-but we don’t have the molecular scale information in the fuel cell,” Hickner says. “That’s the next step, trying to figure out how these polymers are working in the fuel cell on a detailed level.”
The Advanced Research Projects Agency-Energy at the US Department of Energy funded this project in collaboration with Proton OnSite, a leading membrane electrolyzer company based in Connecticut.
Image caption – An example membrane. The cost-efficient and durable alternative for fuel cells consists of two electrodes with a clear membrane sandwiched between them. Courtesy of Patrick Mansell/Penn State.
More information: