Skip to content

Treibacher suspension plasma spray study compares spray rates of higher solids for TBC

Engineers from Treibacher Industrie AG, Austria, present Suspension Spray for Thermal Barrier Coatings – Expanding the Envelope, a report on efforts to expand the application of suspension plasma spray for thermal barrier coatings in gas turbines at the International Thermal spray conference in Florida.

Suspension plasma spray has become an industrially accepted coating method in recent years. The aerospace certification of suspensions demonstrates the advances that have been made since the technique was first developed.

Although the first coatings are entering service, further development of the process is needed to expand is use within the gas turbine. High-solids load suspensions have been used to produce TBC coatings at spray rates comparable to powder spraying. However, it has yet to be demonstrated that these coatings improve upon the properties of standard suspension coatings.

This study has focused on the comparison between an industry standard suspension used for production, and higher solids load suspensions formulated with ethanol and aqueous-based solvents. The coating process has been customized for each suspension to obtain a coating with the required columnar or highly segmented structure. The coating processes have been compared in terms of spray rate and deposition efficiency to assess their impact on production. The coatings produced from each suspension have been characterized for their properties in terms of thermo-cyclic fatigue lifetime. The thermal conductivity of the coatings has been measured in their as produced state as well as after exposure to high temperatures.

Monday, May 7, 2018: 9:40 AM

Tampa 1 (Gaylord Palms Resort )

Dr. Nicholas Curry , Treibacher Industrie AG, Althofen, Austria

Learn more: https://staging.asminternational.org/web/itsc-2018/home 