Researchers use nanoparticles to increase light frequency and resolution of imaging systems
May 18, 2023 Source: ASM International
Physicists at the Australian National University (ANU) are using nanoparticles to develop new sources of light that increase the frequency of light that cameras and other technologies see by up to seven times. The researchers say there is “no limit” to how high the frequency of light can be increased. The higher the frequency, the smaller the object that can be seen with this new light source.
The technology, which requires only a single nanoparticle to work, could be implemented into microscopes to help scientists zoom into the world of super small things at 10 times the resolution of conventional microscopes. This would enable researchers to study objects that would otherwise be too small to see, such as the inner structures of cells and individual viruses.
Being able to analyze such small objects could help scientists better understand and fight certain diseases and health conditions. The findings, published in Science Advances, could have major implications for medical science by offering an affordable and effective solution to analyze tiny objects that are too small for microscopes to see, let alone the human eye. The work could also be beneficial for the semiconductor industry and improving quality control of the fabrication of computer chips.
“Conventional microscopes are only able to study objects bigger than about a ten-millionth of a meter. However, there is growing demand across a range of sectors, including the medical field, to be able to analyze much smaller objects down to one billionth of a meter,” lead author Dr. Anastasiia Zalogina, from the ANU Research School of Physics and the University of Adelaide, said. “Our technology could help meet that demand.”
The researchers say the ANU-developed nanotech could help create a new generation of microscopes that can produce much more detailed images.
“Scientists who want to generate a highly-magnified image of an extremely small, nanoscale object can’t use a conventional optical microscope. Instead, they must rely on either super-resolution microscopy techniques or use an electron microscope to study these tiny objects,” Dr. Zalogina said.
“But such techniques are slow and the technology is very expensive, often costing more than a million dollars. Another disadvantage of electron microscopy is that it may damage delicate samples being analyzed, whereas light-based microscopes mitigate this issue.”
Beams of light that we perceive as different colors of the rainbow are electromagnetic waves that oscillate with different frequencies.
What we see as red is the lowest frequency that our eyes can detect. Even lower frequencies not visible to the human eye are called infra-red. Violet has the highest light frequency that we can see. Ultraviolet, which has an even higher frequency, is invisible to the human eye. Although our eyes cannot detect infra-red and ultraviolet light, it is possible for us to “see” it using cameras and other technologies.
Co-author Dr. Sergey Kruk, also from ANU, said researchers are interested in achieving very high frequencies of light, also known as extreme-ultraviolet. “With violet light we can see much smaller things compared to using red light. And with extreme-ultraviolet light sources we can see things beyond what’s possible using conventional microscopes of today,” Dr. Kruk said.
The ANU technology could also be used in the semiconductor industry as a quality control measure to ensure a streamlined manufacturing process. “Computer chips consist of very tiny components with feature sizes almost as small as one billionth of a meter. During the chip production process, it would be beneficial for manufacturers to use tiny sources of extreme-ultraviolet light to monitor this process in real-time to diagnose any problems early on,” he said.
Image – Courtesy of: Unsplash/CC0 Public Domain.
For more information:
Australian National University
Subject Classifications
Inspection
materials characterization
Materials Testing and Evaluation
Nanotechnology
news
News Articles
Testing and Monitoring
Tests and Diagnostics