Seeing inside next-generation microelectronics using X-rays
June 19, 2025 Source: ASM International
As electronics become smaller, researchers are designing new devices using novel nanoscale materials. These materials have new structures, such as ultra-thin layered “nanosheets.” Understanding the inner details of these tiny devices helps researchers use them in microelectronics. However, the devices’ small size makes it very difficult to examine them in a way that doesn’t destroy their initial structure.
U.S. Department of Energy scientists used an X-ray beam with a diameter of just 12 nanometers to “see” the details of the nanosheets’ structures without damaging them. The experiments revealed two competing mechanisms that contribute to how deformations occur in these nanosheets.
Consumers want electronics that are ever smaller and faster. But the fabrication methods industry and researchers use to create tiny, high-power electronics are complex and can cause the nanostructures to have unwanted defects and deformations. Understanding these inner details—and doing so in a way that doesn’t cause further damage—is essential to determining how to use nanostructures in real-world applications. This study provides a non-destructive method for studying materials that yields insights into the structure of these devices at the nanoscale. It also opens a new avenue for developing novel nanoscale structures for electronics applications.
Nanosheets are used in tiny next-generation electronic components called Gate-All-Around Field Effect Transistors (GAAFETs). These components form the basis of computer microprocessors at the heart of smartphones and computers. In this study, a team of researchers from IBM collaborated with scientists from the National Synchrotron Light Source II (NSLS-II), a Department of Energy Office of Science user facility at Brookhaven National Laboratory, to map the deformations within nanosheets. The researchers investigated these structures using the Hard X-ray Nanoprobe (HXN) beamline at the NSLS-II light source.
By exploiting the brilliant source of X-rays and the resolving power provided by a nanofocusing optics setup called a multilayer Laue lens, the researchers were able to identify two competing mechanisms at different length scales that contribute to the deformation. The first, which is long-range and previously known, is due to the mismatch of lattice constant between the different elements and a relaxation effect near edges. The second, a much shorter-range effect, is associated with the layering itself and is dominant within a length scale of the nanosheet thickness from the edge. These new insights could help researchers predict essential performance parameters of future devices, such as the carrier mobility.
Image – Artist’s impression of how X-rays make it possible to study the distortions of the layers in the microelectronics material. The atoms at the edges of the layers are either squished tighter or pulled apart, creating a bend along the different layers. Courtesy of: Brookhaven National Laboratory.
For more information:
U.S. Department of Energy Office of Science
https://www.energy.gov/science/office-science
Subject Classifications
Electronics and Microelectronics
Failure Analysis
materials characterization
Microelectronic Failure Analysis
news
News Articles
Nondestructive Testing