TOPCon modules endure ‘significant degradation’ in damp heat testing compared to PERC
May 9, 2024 Source: ASM International
Scientists from the University of New South Wales published a report into passivated emitter and rear contact (PERC) and tunnel oxide passivated contact (TOPCon) solar modules, finding that the latter has endured “significant degradation” in damp heat testing.
The results of the study were published in the report, ‘Buyer aware: Three new failure modules in TOPCon modules absent from PERC technology’. The researchers tested a range of both TOPCon and PERC modules, with varying components, such as polyolefin elastomer and ethyl-vinyl acetate, to determine how exposure to damp heat environments could affect the modules’ performance.
They found that variations in components made little difference to the performance of the modules in this environment, but that the use of TOPCon versus PERC technology made a significant difference. Over 1,000 hours of testing in damp heat environments, PERC modules endured a maximum power loss of just 1-2% relative, compared to a much higher, and wider-ranging, power loss of 4-65% relative in TOPCon modules.
The team suggested that “electrochemical reactions involving moisture” were likely to blame for the poor performance among TOPCon modules, with three types of failures observed among TOPCon modules: point-localised failure, failure at the connection point of ribbons and busbars and failure throughout “the whole area of cells [and] modules”.
While the researchers noted that the specific contaminant responsible for this decline in output is “unclear at present”, they speculated that the presence of sodium and chlorine on solar modules, transmitted from human fingertips during assembly and transportation, could have an effect on TOPCon cell, which were “found to be particularly vulnerable”.
This could be a significant development as TOPCon modules are expected to become more commonplace in the global solar sector. Vitor Rodrigues, technical director of Iberia and Latin America at GCL SI, spoke at the 2024 Large Scale Solar Europe summit in London in May, and announced that “PERC will start to disappear” in 2024 as developers shift their focus from PERC to other technologies, such as TOPCon.
“Urgent and extensive research efforts are crucial to substantially increase our comprehension and fortify the reliability of TOPCon cells against the pernicious effects of moisture and other contaminants,” wrote the researchers in the report, highlighting the importance of further research into the performance of TOPCon modules in humid environments.
Image – Images of TOPCon modules taken before and after 1,000 hours of damp heat testing (left) and the electroluminescence image ratio of TOPCon modules. Courtesy of: University of New South Wales, Solar Energy Materials and Solar Cells.
For more information:
University of New South Wales
Subject Classifications
electrical-properties
Environmental Impacts
Failure Analysis
High-temperature environments
Materials Properties and Performance
news
News Articles
Problems and Troubleshooting
Renewable Energy
Research and Development
Testing and Characterization